Category: | Polyolefin, Unspecified , Polyolefin |
Manufacturer: | Crosspolimeri S.p.A. |
Trademark: | FRAGOM |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | P0qZxT_FRAGOM-PR-6-92.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
FRAGOM is the trade-mark of our flame retardant halogen free polyolefine thermoplastic compounds FRAGOM PR/6 92 is a flame retardant polyolefine thermoplastic compound having high temperature index and good oxygen index, suitable for cable sheathing and insulation. Certify: CEI 2011TM9,CEI 2022 II/III |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.48 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (190°C/21.6 kg) | 8.0 | g/10 min | ASTM D1238 |
Water Absorption - 24 hr (100°C) | 13.0 | g/m² | IEC 60811 |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Hot Pressure Test - Penetration 1(80°C) | 30 | % |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Corrosive Gas in Smoke - pH | > 4.30 | IEC 60754-2 | |
Halogen Content | < 0.300 | % | IEC 60754-1 |
Temperature Index (Burning) 2 | > 330 | °C | NES 715 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D) | 51 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield) | 14.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 180 | % | ISO 527-2 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (100°C, 168 hr) | 20 | % | IEC 60811 |
Change in Tensile Strain at Break in Air (100°C, 168 hr) | -18 | % | IEC 60811 |
Change in Tensile Stress | ISO 1817 | ||
23°C, 4 hr, in Gasoline | -18 | % | |
70°C, 4 hr, in SAE 20 Oil | -20 | % | |
Change in Tensile Strain at Break | ISO 1817 | ||
23°C, 4 hr, in Gasoline | 5.0 | % | |
70°C, 4 hr, in SAE 20 Oil | 2.5 | % |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+14 | ohms·cm | BS 6622 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Oxygen Index | 37 | % | ASTM D2863 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 120 | °C | |
Cylinder Zone 2 Temp. | 150 | °C | |
Cylinder Zone 3 Temp. | 160 | °C | |
Cylinder Zone 4 Temp. | 170 | °C | |
Cylinder Zone 5 Temp. | 180 | °C | |
Die Temperature | 185 | °C |
Note Message | |
---|---|
1 . | 4 hr |
2 . | 21% O2 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PrimoPrene 80A-1000 | KMI Group Inc. | TPV | PrimoPrene |
Resiprene® 1030 | Resirene, S.A. de C.V. | TPE | Resiprene® |
Starflam PX06020 | Eurostar Engineering Plastics | Nylon 6 | Starflam |
UNIBRITE® UB-830 | Nippon A&L Inc. | AES | UNIBRITE® |
Edgetek™ PK-30GF/000 NC | PolyOne Corporation | PEEK | Edgetek™ |