| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Solvay Engineering Plastics |
| Trademark: | TECHNYL® A |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Oxc6Z0_TECHNYL-A-208K-BLACK-10N-L.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Polyamide 66, Highly UV-resistance, toughness modified for injection molding |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Uses |
|
| Appearance |
|
| Processing Method |
|
| Part Marking Code (ISO 11469) |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.14 | -- | g/cm³ | ISO 1183 |
| Molding Shrinkage | Internal Method | |||
| Across Flow | 1.9 | -- | % | |
| Flow | 1.9 | -- | % | |
| Water Absorption (Equilibrium, 23°C, 50% RH) | 1.2 | -- | % | ISO 62 |
| Hardness | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Rockwell Hardness (R-Scale) | 121 | -- | ASTM D785 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Strength (Yield) | 84.0 | -- | MPa | ASTM D638 |
| Tensile Elongation (Break) | 10 | -- | % | ASTM D638 |
| Flexural Modulus | 3000 | -- | MPa | ASTM D790 |
| Flexural Strength (Break) | 118 | -- | MPa | ASTM D790 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Notched Izod Impact | 62 | -- | J/m | ASTM D256 |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Deflection Temperature Under Load | ASTM D648 | |||
| 0.45 MPa, Unannealed | 73.0 | -- | °C | |
| 1.8 MPa, Unannealed | 211 | -- | °C | |
| Melting Temperature | 262 | -- | °C | ISO 11357-3 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Surface Resistivity | 1.0E+14 | 4.0E+12 | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+15 | 1.0E+14 | ohms·cm | IEC 60093 |
| Relative Permittivity | 2.90 | 3.20 | IEC 60250 | |
| Dissipation Factor | 0.030 | 0.080 | IEC 60250 |
| Injection | Dry | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Suggested Max Moisture | 0.20 | % | |
| Rear Temperature | 265 to 285 | °C | |
| Middle Temperature | 270 to 290 | °C | |
| Front Temperature | 275 to 295 | °C | |
| Mold Temperature | 50.0 to 80.0 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| NAXALOY® 774 | MRC Polymers, Inc. | PC+ABS | NAXALOY® |
| ARMAMID® PA NE 30-1E | Poly Plastic | Nylon 6 | ARMAMID® |
| EZPrene 9555A SHF | ENPLAST Americas, a Ravago Group Company | TPV | EZPrene |
| KOPELEN JM-375 | Lotte Chemical Corporation | PP Impact Copolymer | KOPELEN |
| Huafon JF-W-BK3045 | Huafon Group Co., Ltd. | PUR, Unspecified | Huafon |