Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL® C |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | OgGdgI_TECHNYL-C-218-V40-BLACK-21.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TECHNYL C 218 V40 is a polyamide 6 with 40% of glass fiber and with thermal stability. |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Appearance |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Specific Gravity | 1.45 | -- | g/cm³ | ASTM D792 |
Water Absorption (Equilibrium, 23°C, 50% RH) | 0.90 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 13100 | 7300 | MPa | ISO 527-2 |
Tensile Stress (23°C) | 210 | 140 | MPa | ISO 527-2 |
Tensile Strain (Break, 23°C) | 2.3 | 3.5 | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 18 | 34 | kJ/m² | ISO 179 |
Charpy Unnotched Impact Strength (23°C) | 110 | 120 | kJ/m² | ISO 179 |
Notched Izod Impact Strength (23°C) | 16 | 34 | kJ/m² | ISO 180 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 214 | -- | °C | ISO 75-2/A |
Peak Melting Temperature | 222 | -- | °C | ASTM D3418 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Volume Resistivity (23°C) | 1.0E+15 | 1.0E+11 | ohms·cm | IEC 60093 |
Electric Strength (23°C) | -- | 22 | kV/mm | IEC 60243-1 |
Relative Permittivity (23°C, 1 MHz) | 3.80 | 4.50 | IEC 60250 | |
Dissipation Factor (23°C, 1 MHz) | 0.020 | 9.0E-3 | IEC 60250 | |
Comparative Tracking Index | 550 | 475 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating | HB | -- | UL 94 | |
Glow Wire Flammability Index (1.60 mm) | 650 | -- | °C | IEC 60695-2-12 |
Oxygen Index | 23 | -- | % | ISO 4589-2 |
Injection | Dry | Unit | |
---|---|---|---|
Rear Temperature | 240 to 260 | °C | |
Middle Temperature | 230 to 240 | °C | |
Front Temperature | 240 to 250 | °C | |
Nozzle Temperature | 230 to 240 | °C | |
Mold Temperature | 80.0 to 100 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
THERMOLAST® K TC6HBA (Series: AD/POM) | KRAIBURG TPE | TPE | THERMOLAST® K |
XAREC™ S834 | Idemitsu Kosan Co., Ltd. | SPS | XAREC™ |
ADDILENE J 120 M20 | ADDIPLAST | PP Copolymer | ADDILENE |
EMERGE™ PC 8410-10 | Trinseo | PC | EMERGE™ |
ENVIROPLAS® ENV00-NC670 | ENVIROPLAS®, Inc. | ABS | ENVIROPLAS® |