| Category: | PP+EPDM , Polypropylene + EPDM Rubber |
| Manufacturer: | Polykemi AB |
| Trademark: | POLYelast |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Oe09EC_POLYelast-TPE-EC90-D50-P05B.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| PP/EPDM |
| General Information |
|---|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.930 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 12 | g/10 min | ISO 1133 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 1.2 to 1.5 | % | |
| Flow | 1.2 to 1.5 | % |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D, 15 sec) | 55 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 15.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 300 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 650 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -30°C | 15 | kJ/m² | |
| 23°C | 30 | kJ/m² |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1(0.45 MPa, Unannealed) | 87.0 | °C | ISO 75-2/B |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Premier LH01019 - BP | Premier Polymers, LLC. | LLDPE | Premier |
| Shuman PC 980-05V0 | Shuman Plastics, Inc. | PC | Shuman PC |
| VESTOSINT® 2178 white | Evonik Industries AG | Nylon 12 | VESTOSINT® |
| Elastollan® 1185A10 | BASF Corp. Thermoplastic Polyurethanes | TPU-Polyether | Elastollan® |
| POLYfill PPC TS20020 | Polykemi AB | PP Copolymer | POLYfill |