| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | Wellamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | OdG9zG_Wellamid-GF33-66-6-XE-BKDX9.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Wellamid® GF33-66/6 XE-BKDX9 is a Polyamide 66 (Nylon 66) material filled with 33% glass fiber. It is available in Asia Pacific, Europe, Latin America, or North America. Typical application of Wellamid® GF33-66/6 XE-BKDX9: Automotive |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Appearance |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.40 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow : 23°C | 0.80 to 1.2 | % | |
| Flow : 23°C | 0.20 to 0.60 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 180 | MPa | ISO 527-2 |
| Tensile Strain (Yield, 23°C) | 3.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 9500 | MPa | ISO 178 |
| Flexural Stress (23°C) | 250 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 10 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 210 | °C | ISO 75-2/A |
| Melting Temperature (DSC) | 260 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RJM SI302G30 | RJM International, Inc. | PET | RJM |
| VESTAMID® Care ME55-B | Evonik Industries AG | PEBA-Ether | VESTAMID® Care |
| Niuk 60GP30 | Shanghai Niuk New Plastic Technology Co., Ltd. | PBT | Niuk |
| Delrin® FG100P NC010 | DuPont Performance Polymers | Acetal (POM) Homopolymer | Delrin® |
| Polimid A 30 GF V0A | Poliblend S.p.a. | Nylon 66 | Polimid A |