| Category: | PP, Unspecified , Polypropylene |
| Manufacturer: | Putsch Kunststoffe GmbH |
| Trademark: | Prop |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | OagweC_Prop-6002.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Prop 6002 is a polypropylene product,. It is available in Europe. |
| General Information |
|---|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.900 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 12 | g/10 min | ISO 1133 |
| Molding Shrinkage | 1.5 - 2.0 | % | Internal method |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ISO 527-2 | ||
| Yield | 24.0 | MPa | ISO 527-2 |
| Fracture | 21.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 20 | % | ISO 527-2 |
| Flexural Modulus | 1400 | MPa | ISO 178 |
| Flexural Stress (3.5% Strain) | 52.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact | ISO 180 | ||
| -20°C | 3.5 | kJ/m² | ISO 180 |
| 23°C | 6.0 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 72.0 | °C | ISO 306/B |
| Additional Information |
|---|
| Tensile Strength, ISO 527: 24 MPa |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Processing (Melt) Temp | 210 - 230 | °C | |
| Mold Temperature | 20.0 - 40.0 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Menzolit® SMC 1000 | Menzolit Ltd (UK) | Polyester, TS | Menzolit® |
| Ablebond 84-1LMI | Henkel Ablestik | Epoxy | Ablebond |
| EnCom PPE-PA 2030GF BK43001 | EnCom, Inc. | Nylon+PPE | EnCom |
| PENTAMID B GV30 H RC schwarz | PENTAC Polymer GmbH | Nylon 6 | PENTAMID B |
| Bergadur™ PB40 G15 Natural TM-Y | PolyOne Corporation | PBT | Bergadur™ |