Category: | Nylon 66 Alloy , Polyamide 66 Alloy |
Manufacturer: | Technical Polymers, LLC |
Trademark: | Domamid XS™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | OVaWsZ_DomamidXS5750R50H2.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
PA66 Alloy, 50% Glass Fiber, Heat Stabilized Processing Method: Injection Molding |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.60 | g/cm³ | ISO 1183 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (23°C) | 18000 | MPa | ISO 527-2 |
Tensile Stress (23°C) | 250 | MPa | ISO 527-2 |
Tensile Strain (Break, 23°C) | 2.0 - 4.0 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 15 | kJ/m² | ISO 179 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 235 | °C | ISO 75-2/A |
Melting Temperature (DSC) | 260 | °C | ISO 3146 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | > 1.0E+12 | ohms·cm | ISO 3915 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 75 - 80 | °C | |
Processing (Melt) Temp | 280 - 305 | °C | |
Mold Temperature | 70 - 100 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
WACKER SilGel® 613 A/B | Wacker Chemie AG | Silicone | WACKER SilGel® |
DOW™ HDPE DMDA-8950 NT 7 | The Dow Chemical Company | HDPE | DOW™ HDPE |
BESTNYL SI20VI02AU | Triesa Plastics | Nylon 6 | BESTNYL |
KOCETAL® K500 | Kolon Plastics, Inc. | Acetal (POM) Copolymer | KOCETAL® |
Sylvin 802-88 Yellow 433 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |