| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Teknor Apex Company (Chem Polymer) |
| Trademark: | Chemlon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | OMt3ox_Chemlon-282.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Chemlon® 282 is a Polyamide 6 (Nylon 6) material. It is available in Asia Pacific, Europe, or North America for injection molding. Important attributes of Chemlon® 282 are:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.18 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (235°C/1.0 kg) | 13 | g/10 min | ASTM D1238 |
| Molding Shrinkage - Flow | 0.90 to 1.4 | % | ASTM D955 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (R-Scale) | 120 | ASTM D785 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 72.4 | MPa | ASTM D638 |
| Tensile Elongation | ASTM D638 | ||
| Yield | 6.0 | % | |
| Break | 6.0 | % | |
| Flexural Modulus | 3140 | MPa | ASTM D790 |
| Flexural Strength | 96.5 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 53 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Unannealed) | 79.4 | °C | ASTM D648 |
| Melting Temperature | 216 | °C | DSC |
| RTI Elec | UL 746 | ||
| 0.810 mm | 130 | °C | |
| 1.50 mm | 130 | °C | |
| 3.00 mm | 130 | °C | |
| RTI Imp | UL 746 | ||
| 0.810 mm | 105 | °C | |
| 1.50 mm | 105 | °C | |
| 3.00 mm | 105 | °C | |
| RTI Str | UL 746 | ||
| 0.810 mm | 120 | °C | |
| 1.50 mm | 120 | °C | |
| 3.00 mm | 120 | °C |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 1.0E+15 | ohms·cm | ASTM D257 |
| Dielectric Strength (3.00 mm) | 15 | kV/mm | ASTM D149 |
| Comparative Tracking Index (CTI) | 600 | V | UL 746 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (0.630 mm) | V-0 | UL 94 | |
| Oxygen Index | 32 | % | ASTM D2863 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 79.4 | °C | |
| Suggested Max Moisture | 0.20 | % | |
| Suggested Max Regrind | 25 | % | |
| Rear Temperature | 218 to 235 | °C | |
| Middle Temperature | 229 to 252 | °C | |
| Front Temperature | 241 to 260 | °C | |
| Nozzle Temperature | 241 to 260 | °C | |
| Processing (Melt) Temp | 241 to 260 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 2181 HEC HF | RTP Company | PEI | RTP |
| Escorene™ Ultra UL 02528CC | ExxonMobil Chemical | EVA | Escorene™ Ultra |
| Filter-bond™ R-30-6-1 | Hapco Inc. | TS, Unspecified | Filter-bond™ |
| LEXAN™ OQ3732 resin | SABIC Innovative Plastics Europe | PC | LEXAN™ |
| OP - PC - Filled 30GF | Oxford Polymers | PC | OP - PC - Filled |