| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | BASF Corp. Thermoplastic Polyurethanes |
| Trademark: | Elastollan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | OMGU1Y_Elastollan-C59D.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Elastollan® C59D exhibits excellent abrasion resistance and toughness, good hydrolytic stability, good heat, oil, fuel and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® C59D is rated UL-94 V-2 in vertical flame test for wall thickness of 0.75 mm. Elastollan® C59D is supplied uncolored in diced form. |
| General Information | |
|---|---|
| Features |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.23 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 56 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus (Injection Molded) | 131 | MPa | ASTM D412 |
| Flexural Modulus (Injection Molded) | 138 | MPa | ASTM D790 |
| Taber Abrasion Resistance | 45.0 | mg | ASTM D1044 |
| Abrasion - DIN | 25 | mm³ | DIN 53516 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Softening Point - DMA | 131 | °C | Internal Method |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 100% Strain | 23.4 | MPa | |
| 300% Strain | 46.2 | MPa | |
| Tensile Strength | 50.3 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 430 | % | ASTM D412 |
| Tear Strength 1 | 210 | kN/m | ASTM D624 |
| Compression Set | ASTM D395B | ||
| 23°C, 22 hr | 30 | % | |
| 70°C, 22 hr | 50 | % |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glass Transition Temperature | -15.0 | °C | Internal Method |
| Vicat Softening Temperature | 143 | °C | ASTM D1525 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating (0.750 mm) | V-2 | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 110 to 120 | °C | |
| Drying Time | 2.0 to 3.0 | hr | |
| Suggested Max Moisture | 0.030 | % | |
| Rear Temperature | 210 to 230 | °C | |
| Middle Temperature | 210 to 230 | °C | |
| Front Temperature | 210 to 230 | °C | |
| Nozzle Temperature | 220 to 240 | °C |
| Note Message | |
|---|---|
| 1 . | Die C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Radilon® S 24E 100 NAT | Radici Plastics | Nylon 6 | Radilon® |
| Purell ACP 6541A | LyondellBasell Industries | HDPE | Purell |
| Zeoforte® ZSC2095 | Zeon Corporation | NBR | Zeoforte® |
| Delrin® 127UVE NC010 | DuPont Performance Polymers | Acetal (POM) Homopolymer | Delrin® |
| LNP™ LUBRICOMP™ UFL36AS compound | SABIC Innovative Plastics | PPA | LNP™ LUBRICOMP™ |