Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Oxford Polymers |
Trademark: | OXNILON 6 |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | OLrMRN_OXNILON-6-14GF.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
OXNILON 6 14GF is a Polyamide 6 (Nylon 6) material filled with 14% glass fiber. It is available in North America for injection molding. |
General Information | |
---|---|
Filler / Reinforcement |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.23 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow | 0.50 | % | ASTM D955 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Yield) | 110 | MPa | ASTM D638 |
Tensile Elongation (Break) | 3.0 | % | ASTM D638 |
Flexural Modulus | 5170 | MPa | ASTM D790 |
Flexural Strength | 152 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 53 | J/m | ASTM D256 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load (1.8 MPa, Unannealed) | 199 | °C | ASTM D648 |
Melting Temperature | 219 | °C |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 79.4 | °C | |
Drying Time | 2.0 to 4.0 | hr | |
Rear Temperature | 249 to 277 | °C | |
Middle Temperature | 260 to 288 | °C | |
Front Temperature | 268 to 296 | °C | |
Nozzle Temperature | 268 to 296 | °C | |
Processing (Melt) Temp | 260 to 271 | °C | |
Mold Temperature | 65.6 to 124 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Rilsamid® AZM 30 GT8LD | Arkema | Nylon 12 | Rilsamid® |
TECHNYL® A 218 V50 BLACK 21 N | Solvay Engineering Plastics | Nylon 66 | TECHNYL® A |
Witcobond® W-281F | Chemtura | PUR-Ester | Witcobond® |
Generic PPA - Glass Fiber, Long | Generic | PPA | Generic |
ESTABLEND 0840 GF | Cossa Polimeri S.r.l. | PC+ABS | ESTABLEND |