Category: | PEEK , Polyetheretherketone |
Manufacturer: | Polymer Dynamix |
Trademark: | DynaMix™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | OLOIob_DynaMix-3204-HF.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Modified PEEK Features:
Applications:
|
General Information | |
---|---|
Features |
|
Uses |
|
Processing Method |
|
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | ASTM D638 | ||
Yield | 79.3 | MPa | |
Break | 80.0 | MPa | |
Tensile Elongation | ASTM D638 | ||
Yield | 5.0 to 6.0 | % | |
Break | 20 to 30 | % | |
Flexural Modulus | 3450 | MPa | ASTM D790 |
Flexural Strength | 138 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C, 3.18 mm) | 91 | J/m | ASTM D256 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 121 to 149 | °C | |
Drying Time | 3.0 to 5.0 | hr | |
Rear Temperature | 332 to 360 | °C | |
Middle Temperature | 338 to 366 | °C | |
Front Temperature | 343 to 377 | °C | |
Nozzle Temperature | 343 to 377 | °C | |
Processing (Melt) Temp | 343 to 377 | °C | |
Mold Temperature | 177 to 204 | °C | |
Injection Rate | Moderate | ||
Screw Speed | 40 to 70 | rpm | |
Clamp Tonnage | 4.1 to 6.9 | kN/cm² |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
THERMOLAST® K TC6CSZ (Series: CS) | KRAIBURG TPE | TPE | THERMOLAST® K |
Multi-Flex® TPE D3604 | Multibase, A Dow Corning Company | TPE | Multi-Flex® TPE |
APEX® 94-A0907N-86NT | Teknor Apex Company | PVC, Flexible | APEX® |
ECOMID A GF30 | Nilit Plastics | Nylon 66 | ECOMID |
Pearlthane® CLEAR 15N80 | Lubrizol Advanced Materials, Inc. | TPU-Polyether | Pearlthane® |