Category: | Fluorelastomer , Fluoroelastomer |
Manufacturer: | Greene, Tweed & Co. |
Trademark: | Greene FKM |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | O5azEP_Greene-FKM-929.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Greene FKM 929 is a Fluoroelastomer product. It is available in North America. |
General Information | |
---|---|
Appearance |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.85 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shore A | 97 | ||
Shore D | 65 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Break) | 18.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 26 | % | ASTM D412 |
Compression Set 1 | ASTM D395 | ||
100°C, 70 hr | 34 | % | |
177°C, 70 hr | 51 | % |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air | ASTM D573 | ||
100°C, 70 hr | -10 | % | |
177°C, 70 hr | -5.0 | % | |
Change in Ultimate Elongation in Air | ASTM D573 | ||
100°C, 70 hr | 11 | % | |
177°C, 70 hr | -9.0 | % | |
Change in Durometer Hardness in Air | ASTM D573 | ||
Shore A, 100°C, 70 hr | 0.0 | ||
Shore D, 100°C, 70 hr | -3.0 | ||
Shore A, 177°C, 70 hr | 0.0 | ||
Shore D, 177°C, 70 hr | -4.0 | ||
Change in Tensile Strength | ASTM D471 | ||
100°C, 70 hr, in ASTM #1 Oil | -2.0 | % | |
100°C, 70 hr, in ASTM #3 Oil | -4.8 | % | |
177°C, 70 hr, in ASTM #3 Oil | -11 | % | |
Change in Ultimate Elongation | ASTM D471 | ||
100°C, 70 hr, in ASTM #1 Oil | 11 | % | |
100°C, 70 hr, in ASTM #3 Oil | 8.6 | % | |
177°C, 70 hr, in ASTM #3 Oil | 23 | % | |
Change in Durometer Hardness | ASTM D471 | ||
Shore A, 100°C, 70 hr, in ASTM #1 Oil | 0.0 | ||
Shore D, 100°C, 70 hr, in ASTM #1 Oil | -5.0 | ||
Shore A, 100°C, 70 hr, in ASTM #3 Oil | 0.0 | ||
Shore D, 100°C, 70 hr, in ASTM #3 Oil | -5.0 | ||
Shore A, 177°C, 70 hr, in ASTM #3 Oil | -1.0 | ||
Shore D, 177°C, 70 hr, in ASTM #3 Oil | -7.0 | ||
Change in Volume | ASTM D471 | ||
100°C, 70 hr, in ASTM Oil #1 | 0.80 | % | |
100°C, 70 hr, in ASTM Oil #3 | 1.1 | % | |
177°C, 70 hr, in ASTM Oil #3 | 3.2 | % |
Thermal | Nominal Value | Unit | |
---|---|---|---|
Service Temperature | -29 to 204 | °C |
Additional Information | Nominal Value | Unit | Test Method |
---|---|---|---|
Rubber Classification 2 | FKM | ||
Tear Strength - Die C | 41.2 | kN/m | ASTM D624 |
Note Message | |
---|---|
1 . | 25% Deflection |
2 . | ASTM D1418 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PRL PC-FR3A-D-(color)-3 | Polymer Resources Ltd. | PC | PRL |
MIDILENA I LDPE B20/2 | ROMPETROL PETROCHEMICALS S.R.L. | LDPE | MIDILENA I |
TEREZ PA 6 7200 | TER HELL PLASTIC GMBH | Nylon 6 | TEREZ PA 6 |
Exceed™ 1015HA mVLDPE | ExxonMobil Chemical | mPE | Exceed™ |
OTECH TPO OTO9097 - Cord Insulation | OTECH Corporation | TPO | OTECH TPO |