Unreinforced - Flame Retardant - UL94 V-0 |
General Information | |
---|---|
Features |
|
RoHS Compliance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.43 | g/cm³ | ASTM D792 |
Molding Shrinkage - Flow (3.20 mm) | 1.8 - 2.4 | % | ASTM D955 |
Water Absorption (23°C, 24 hr) | 0.080 | % | ASTM D570 |
Moisture Content | 0.030 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale) | 118 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 2960 | MPa | ASTM D638 |
Tensile Strength | 62.1 | MPa | ASTM D638 |
Tensile Elongation (Yield) | 6.0 - 10 | % | ASTM D638 |
Flexural Modulus | 2960 | MPa | ASTM D790 |
Flexural Strength | 103 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (3.20 mm) | 32 | J/m | ASTM D256 |
Unnotched Izod Impact (3.20 mm) | 850 | J/m | ASTM D4812 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, not annealed | 160 | °C | ASTM D648 |
1.8 MPa, not annealed | 71.1 | °C | ASTM D648 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | > 1.0E+16 | ohms·cm | ASTM D257 |
Dielectric Strength 1(in Oil) | 18 | kV/mm | ASTM D149 |
Dielectric Constant (1 MHz) | 3.20 | ASTM D150 | |
Dissipation Factor (1 MHz) | 0.020 | ASTM D150 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (0.800 mm) | V-0 | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 121 | °C | |
Drying Time | 4.0 | hr | |
Dew Point | -28.9 | °C | |
Processing (Melt) Temp | 238 - 271 | °C | |
Mold Temperature | 79.4 - 107 | °C | |
Injection Pressure | 68.9 - 103 | MPa |
Injection instructions |
---|
Desiccant Type Dryer Required. |
Note Message | |
---|---|
1 . | Method A (short time) |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SABIC® PP 522L | Saudi Basic Industries Corporation (SABIC) | PP Homopolymer | SABIC® PP |
Shin-Etsu Elastomer KE-561U | Shin-Etsu Silicones of America | Silicone Rubber, HTV | Shin-Etsu Elastomer |
Sinvicomp STG8501 | Teknor Apex Asia Pacific PTE. LTD. | PVC, Flexible | Sinvicomp |
Celcon® MC90-HM | Celanese Corporation | Acetal (POM) Copolymer | Celcon® |
Clariant PC PC-1100 | Clariant Corporation | PC | Clariant PC |