Category: | Nylon 46 , Polyamide 46 |
Manufacturer: | Comco-Plastic GmbH |
Trademark: | Comco |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | NmSVc8_Comco-PA-4-6.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Comco PA 4.6 is a Polyamide 46 (Nylon 46) material. It is available in Europe. Primary attribute of Comco PA 4.6: Flame Rated. |
General Information | |
---|---|
Appearance |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.18 | -- | g/cm³ | ISO 1183 |
Water Absorption | ||||
Saturation, 23°C | 9.5 | -- | % | |
Equilibrium, 23°C, 50% RH | 2.8 | -- | % | |
Water Absorption | ISO 62 | |||
after 24 h immersion in water : 23°C | 90.0 | -- | mg | |
after 96 h immersion in water : 23°C | 180.0 | -- | mg |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Maximum Service Temperature | ||||
in air continuosly | 155 | -- | °C | |
in air for short periods | 200 | -- | °C | |
Service Temperature - Minimum | -40 | -- | °C |
Hardness | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Rockwell Hardness (M-Scale) | 92 | -- | ISO 2039-2 | |
Ball Indentation Hardness | 165 | -- | MPa | ISO 2039-1 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 3300 | 1300 | MPa | ISO 527-2 |
Tensile Stress (Yield, 23°C) | 100 | 55.0 | MPa | ISO 527-2 |
Tensile Strain (Break, 23°C) | 25 | > 100 | % | ISO 527-2 |
Tensile Creep Modulus 1(1000 hr) | 22.0 | 7.50 | MPa | ISO 899-1 |
Compressive Stress | ISO 604 | |||
5% Strain | 94.0 | -- | MPa | |
2% Strain | 45.0 | -- | MPa | |
1% Strain | 23.0 | -- | MPa |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | 8.0 | -- | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | No Break | -- | ISO 179/1eU | |
Notched Izod Impact Strength | 8.0 | 25 | kJ/m² | ISO 180/2A |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 160 | -- | °C | ISO 75-2/A |
Melting Temperature | 295 | -- | °C | |
CLTE - Flow | ||||
23 to 60°C | 8.0E-5 | -- | cm/cm/°C | |
23 to 100°C | 9.0E-5 | -- | cm/cm/°C | |
Thermal Conductivity | 0.30 | -- | W/m/K |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | > 1.0E+13 | > 1.0E+12 | ohms | IEC 60093 |
Volume Resistivity | > 1.0E+14 | > 1.0E+12 | ohms·cm | IEC 60093 |
Electric Strength | 25 | 15 | kV/mm | IEC 60243-1 |
Relative Permittivity | IEC 60250 | |||
100 Hz | 3.80 | 7.40 | ||
1 MHz | 3.40 | 3.80 | ||
Dissipation Factor | IEC 60250 | |||
100 Hz | 9.0E-3 | 0.13 | ||
1 MHz | 0.019 | 0.060 | ||
Comparative Tracking Index | 400 | 400 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating | UL 94 | |||
3.00 mm | HB | -- | ||
6.00 mm | HB | -- | ||
Oxygen Index | 24 | -- | % | ISO 4589-2 |
Note Message | |
---|---|
1 . | 1% Strain |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Smooth-Cast® 385 | Smooth-On, Inc | PUR, Unspecified | Smooth-Cast® |
TITANLENE® LDF 800GG | Lotte Chemical Titan (M) Sdn. Bhd. | LDPE | TITANLENE® |
Evermore PUR SS-1030NHR | Evermore Chemical Industry Co., Ltd. | PUR, Unspecified | Evermore PUR |
ELEVATE™ EF529 | Westlake Chemical Corporation | EVA | ELEVATE™ |
ELASTOSIL® RT 619 A/B | Wacker Chemie AG | Silicone | ELASTOSIL® RT |