Santoprene™ 241-80W236

Category: TPV , Thermoplastic Vulcanizate
Manufacturer: ExxonMobil Chemical
Trademark: Santoprene™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: NlUzTh_Santoprene-241-80W236.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
It is a soft, colorable, special thermoplastic vulcanized elastomer (T PV) in the thermoplastic elastomer (TPE) series. It is suitable for the field of pipeline engineering related to drinking water. This brand of Shanduping TPV is a shear rate dependent product that can be processed on conventional thermoplastic injection molding, extrusion molding, blow molding, thermoforming or vacuum forming equipment. It is a polyolefin-based product and can be completely recycled.
General Information
Features
  • Good dimensional stability
  • Low compressive deformability
  • Flexibility at low temperatures
  • Recyclable materials
  • Good heat aging resistance
  • Good coloring
  • Ozone resistance
  • Good chemical resistance
  • Fatigue resistance
  • Copper contact stability
Uses
  • Pipe components
Agency Ratings
  • NSF 61
RoHS Compliance
  • RoHS compliance
Appearance
  • Natural color
Forms
  • Particle
Processing Method
  • Blow molding
  • Multiple injection molding
  • Co-extrusion molding
  • Extrusion
  • Extrusion blow molding
  • Sheet extrusion molding
  • Thermoforming
  • Profile extrusion molding
  • Vacuum forming
  • Injection blowing molding
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity
    -- 0.958g/cm³ASTM D792
    -- 0.960g/cm³ISO 1183
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shaw A, 15 seconds, 23°C, 2.00mm)87ISO 868
ElastomersNominal ValueUnitTest Method
Tensile Stress - Across Flow (100% Strain, 23°C)4.40MPaASTM D412, ISO 37
Tensile Strength - Across Flow (Break, 23°C)11.0MPaASTM D412, ISO 37
Tensile Elongation - Across Flow (Break, 23°C)560%ASTM D412, ISO 37
Additional Information
如果适用,这是基于扇形浇口注塑成型的平板测试结果。拉伸强度、伸长率和拉伸应力沿垂直流动方向测定 - ISO 1 型,ASTM die C。从埃克森美孚欧洲分支机构直接购买的所有产品都符合 REACH 法规。 对于埃克森 美孚未进口至欧洲的产品,用户应自行评估其是否满足 REACH 法规。
Legal statement
未经埃克森美孚化工书面允许,这种产品包括其产品名称,不得在任何医疗应用领域予以使用或有关详细的产品监管信息,请联系客户服务。
InjectionNominal ValueUnit
Drying Temperature 82.2°C
Drying Time 3.0hr
Suggested Max Moisture 0.080%
Suggested Max Regrind 20%
Rear Temperature 177°C
Middle Temperature 182°C
Front Temperature 188°C
Nozzle Temperature 193 - 232°C
Processing (Melt) Temp 199 - 232°C
Mold Temperature 10.0 - 51.7°C
Injection Rate Fast
Back Pressure 0.345 - 0.689MPa
Screw Speed 100 - 200rpm
Clamp Tonnage 4.1 - 6.9kN/cm²
Cushion 3.18 - 6.35mm
Screw L/D Ratio 16.0:1.0 to 20.0:1.0
Screw Compression Ratio 2.0:1.0 to 2.5:1.0
Vent Depth 0.025mm
Injection instructions
Santoprene TPV与乙缩醛和PVC不相容。更多关于加工和模具设计的信息,请查阅我们的《注射成型指南》小册子和《Santoprene 橡胶的抗铜催化氧化侵蚀性》技术文献。
ExtrusionNominal ValueUnit
Drying Temperature 82.2°C
Drying Time 3.0hr
Melt Temperature 202°C
Die Temperature 204°C
Back Pressure 5.00 - 20.0MPa
Extrusion instructions
Santoprene TPV与乙缩醛和PVC不相容。更多关于加工和模具设计的信息,请查阅我们的《挤出成型指南》和《Santoprene 橡胶的抗铜催化氧化侵蚀性》技术文献。
Resin Grade Manufacturer Category Trademark
OCTAL PET GS 05 OCTAL Holding & Co. PET OCTAL PET
Nylene® 5213 HS Custom Resins Group Nylon 6 Nylene®
Evoprene™ LF 6158 AlphaGary SBC Evoprene™ LF
Elastron® G P.G401.A50.N Elastron USA, Inc. SEBS Elastron® G
Halar® 930LC Solvay Specialty Polymers ECTFE Halar®