| Category: | TPV , Thermoplastic Vulcanizate |
| Manufacturer: | Teknor Apex Company |
| Trademark: | Sarlink® TPV |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | NY4Xhg_Sarlink-TPV-X6170N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Sarlink® TPV X6170N is a Thermoplastic Vulcanizate (TPV) material. It is available in Asia Pacific, Europe, Latin America, or North America. |
| General Information | |
|---|---|
| Appearance |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.929 | g/cm³ | ISO 1183 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness | ISO 868 | ||
| Shore A, 5 sec, Extruded | 72 | ||
| Shore A, 5 sec, Injection Molded | 76 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ISO 37 | ||
| Across Flow : 100% Strain | 3.00 | MPa | |
| Flow : 100% Strain | 4.30 | MPa | |
| Tensile Stress | ISO 37 | ||
| Across Flow : Break | 6.00 | MPa | |
| Flow : Break | 5.40 | MPa | |
| Tensile Elongation | ISO 37 | ||
| Across Flow : Break | 510 | % | |
| Flow : Break | 340 | % | |
| Compression Set (70°C, 22 hr) | 46 | % | ISO 815 |
| Additional Information | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Apparent Shear Viscosity - Capillary 1(200°C) | 165 | Pa·s | ISO 11443 |
| Note Message | |
|---|---|
| 1 . | 206 1/s |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| STABAMID® 27 FE 5 | Solvay Polyamide & Intermediates | Nylon 66 | STABAMID® |
| VITAMIDE® BF23YL6634 | Jackdaw Polymers | Nylon 6 | VITAMIDE® |
| Hanwha Total PP TH52 | HANWHA TOTAL PETROCHEMICALS Co., Ltd. | PP, High Crystal | Hanwha Total PP |
| Jampilen EP340M | Jam Polypropylene Company | PP Copolymer | Jampilen |
| Karina IVORY PVC COMPOUND SDB 35/ 3-LMP | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |