Category: | LDPE , Low Density Polyethylene Resin |
Manufacturer: | ExxonMobil Chemical |
Trademark: | ExxonMobil™ LDPE |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | NOQMCm_ExxonMobil-LDPE-LD-313-NF.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
LD 313.NF is a 3% (mass fraction) vinyl acetate copolymer. The vinyl acetate content of the resin makes it have better heat sealing performance and low temperature toughness than low density polyethylene homopolymer. |
General Information | |
---|---|
Additive |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 2.5 | g/10 min | ASTM D1238 |
Vinyl Acetate Content | 3.0 | wt% | ExxonMobil Method |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
secant modulus | ASTM D882 | ||
1% secant, MD | 154 | MPa | ASTM D882 |
1% secant, TD | 178 | MPa | ASTM D882 |
Tensile Strength | ASTM D882 | ||
MD : Yield | 8.46 | MPa | ASTM D882 |
TD : Yield | 8.27 | MPa | ASTM D882 |
MD : Fracture | 22.1 | MPa | ASTM D882 |
TD : Fracture | 19.1 | MPa | ASTM D882 |
Tensile Elongation | ASTM D882 | ||
MD : Fracture | 170 | % | ASTM D882 |
TD : Fracture | 540 | % | ASTM D882 |
Dart Drop Impact | 120 | g | ASTM D1709A |
Elmendorf Tear Strength | ASTM D1922 | ||
MD | 200 | g | ASTM D1922 |
TD | 120 | g | ASTM D1922 |
Optical | Nominal Value | Unit | Test Method |
---|---|---|---|
Gloss (45°) | 76 | ASTM D2457 | |
Haze | 5.3 | % | ASTM D1003 |
Legal statement |
---|
有关潜在食品接触应用合规信息(例如:FDA、EU、HPFB),请与埃克森美孚化工客户服务代表联系。本产品不宜在医疗应用中使用,亦不应在任何此类应用中使用 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Matrixx TPP1B20 | The Matrixx Group, Inc. | PP, Unspecified | Matrixx |
NEFTEKHIM PE 4430S (30405) | Nizhnekamskneftekhim Inc. | LLDPE | NEFTEKHIM PE |
BR® 154 | Cytec Industries Inc. | Epoxy | BR® |
Alkathene® LD0220MS | Qenos Pty Ltd | LLDPE | Alkathene® |
POLYfill PP CQX30030 RTX | Polykemi AB | PP, Unspecified | POLYfill |