Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
Manufacturer: | API SpA |
Trademark: | apilon 52® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | NMvvlh_apilon-52-TCLE-40.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
apilon 52®TCLE 40 is a thermoplastic polyurethane elastomer (polyether)(TPU-polyether) product,. It can be processed by extrusion or injection molding and is available in Europe. apilon 52®TCLE 40 applications include engineering/industrial accessories, electrical/electronic applications, electrical appliances, tools and home applications. Features include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.12 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A, 15 seconds | 86 | ASTM D2240 | |
Shaw D, 3 seconds | 35 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | ASTM D638 | ||
-- | 35.0 | MPa | ASTM D638 |
100% strain | 6.90 | MPa | ASTM D638 |
300% strain | 12.0 | MPa | ASTM D638 |
Tensile Elongation (Break) | 600 | % | ASTM D638 |
Abrasion Resistance | 50.0 | mm³ | DIN 53516 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength 1 | 94.0 | kN/m | ASTM D624 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (-20°C) | No Break | ASTM D256 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 110 | °C | |
Drying Time | 2.0 | hr | |
Suggested Max Moisture | 0.070 | % | |
Rear Temperature | 180 - 190 | °C | |
Middle Temperature | 185 - 200 | °C | |
Front Temperature | 190 - 215 | °C | |
Nozzle Temperature | 200 - 230 | °C | |
Mold Temperature | 30.0 - 60.0 | °C | |
Injection Pressure | 50.0 - 100 | MPa | |
Injection Rate | Slow-Moderate |
Injection instructions |
---|
Back Pressure: Medium to LowLocking Pressure: High |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 110 | °C | |
Drying Time | 2.0 | hr | |
Suggested Max Moisture | 0.070 | % | |
Cylinder Zone 1 Temp. | 160 - 185 | °C | |
Cylinder Zone 2 Temp. | 170 - 200 | °C | |
Cylinder Zone 3 Temp. | 175 - 210 | °C | |
Cylinder Zone 4 Temp. | 180 - 220 | °C | |
Die Temperature | 170 - 210 | °C |
Extrusion instructions |
---|
L/D Ratio: 20:1 to 30:1Compression Ratio: 1:2.5 to 1:3 |
Note Message | |
---|---|
1 . | Without Notch |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Makrolon® LTG2623 | Covestro - Polycarbonates | PC | Makrolon® |
RTP 399 X 115084 C | RTP Company | PC | RTP |
SCHULADUR庐 A GF 30 FR 2 natural | A. Schulman Europe | PBT | SCHULADUR® |
TYNAB® GL85 | Tyne Plastics LLC. | ABS | TYNAB® |
LNP™ FARADEX™ AS003 compound | SABIC Innovative Plastics | ABS | LNP™ FARADEX™ |