RTP EMI 260.5 H

Category: Nylon 66 , Polyamide 66
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: N7hOVD_RTP-EMI-260-5-H.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Warning: The status of this material is 'Commercial: Limited Issue'

The data for this material has not been recently verified.
Please contact RTP Company for current information prior to specifying this grade.
General Information
Filler / Reinforcement
  • Stainless steel fiber, 5.0% filler by weight
Additive
  • Impact modifier
Features
  • Impact modification
  • Electromagnetic shielding (EMI)
  • Electrostatic discharge protection
  • Antistatic property
Agency Ratings
  • MIL B-81705C
RoHS Compliance
  • Contact manufacturer
Appearance
  • Black
  • Natural color
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.13g/cm³ASTM D792
Molding Shrinkage - Flow (3.18 mm)1.2 - 1.5%ASTM D955
Water Absorption (23°C, 24 hr)1.5%ASTM D570
MechanicalNominal ValueUnitTest Method
Tensile Modulus 2410MPaASTM D638
Tensile Strength 48.3MPaASTM D638
Tensile Elongation (Break)10%ASTM D638
Flexural Modulus 1720MPaASTM D790
Flexural Strength 65.5MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.18 mm)190J/mASTM D256
Unnotched Izod Impact (3.18 mm)1100J/mASTM D4812
ElectricalNominal ValueUnitTest Method
Surface Resistivity 1.0E+6ohmsASTM D257
Volume Resistivity 1.0E+2ohms·cmASTM D257
FlammabilityNominal ValueUnitTest Method
Flame Rating (1.59 mm)HBUL 94
Additional Information
The value listed as Flammability, UL 94, was tested in accordance with RTP test standards.Mold Shrinkage, Linear-Flow, ASTM D-955, 0.25in.: 15-18mil/in.Tensile Elongation@Break, ASTM D-638: >10%Volume Resistivity, ASTM D-257: <1E2 ohm-cmSurface Resistivity, ASTM D-257: <1E6 ohmStatic Decay, Mil B-81705C: <2.0 secondsShielding Effectiveness, ASTM D4935: 30dB
InjectionNominal ValueUnit
Rear Temperature 274 - 288°C
Middle Temperature 274 - 288°C
Front Temperature 274 - 288°C
Mold Temperature 65.6 - 107°C
Injection Pressure 68.9 - 138MPa
Resin Grade Manufacturer Category Trademark
Ravamid® A BK Ravago Group Nylon 66 Ravamid®
Sarlink® TPV 2555 Teknor Apex Company TPV Sarlink® TPV
COSMOPLENE® FS3011E3 TPC, The Polyolefin Company (Singapore) Pte Ltd PP Homopolymer COSMOPLENE®
Sylvin 6920X08 Grey 9550 Sylvin Technologies Incorporated PVC, Unspecified Sylvin
Sylvin 9077-70 LMW Black Sylvin Technologies Incorporated PVC, Unspecified Sylvin