| Category: | HDPE , High Density Polyethylene |
| Manufacturer: | Osterman & Company |
| Trademark: | Osterlene® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | N2PGN7_OsterleneHB0554.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.952 | g/cm³ | ASTM D4883 |
| Melt Mass-Flow Rate (MFR) | ASTM D1238 | ||
| 190°C/2.16 kg | < 0.10 | g/10 min | ASTM D1238 |
| 190°C/2.16 kg 1 | 5.5 | g/10 min | ASTM D1238 |
| Environmental Stress-Cracking Resistance (100% Igepal) | > 1000 | hr | ASTM D1693 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield) | 28.3 | MPa | ASTM D638 |
| Flexural Modulus | 1380 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Impact Strength (23°C) | 357 | kJ/m² | ASTM D1822 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | < -85.0 | °C | ASTM D746 |
| Vicat Softening Temperature | 126 | °C | ASTM D1525 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Note Message | |
|---|---|
| 1 . | High Load |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP ESD 1700 | RTP Company | PPE+PS | RTP |
| ENVIRON® ENV39-NC450 | ENVIROPLAS®, Inc. | PC+PBT | ENVIRON® |
| KOPET® KP133G30 | Kolon Plastics, Inc. | PET | KOPET® |
| KumhoSunny PC 3603 | Shanghai KumhoSunny Plastics Co., Ltd. | PC | KumhoSunny PC |
| Sylvin 2944-85 Clear Blue 8412 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |