| Category: | HDPE , High Density Polyethylene |
| Manufacturer: | KMI Group, Inc. |
| Trademark: | KMI PE |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | MvMLMU_KMIPEKM104075TL.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
KM 104075TL High Density Polyethylene Characteristics: Generally used for large containers, durable goods, and seating. It is resistant to environmental stress crack, and it has good stiffness. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.949 | g/cm³ | ASTM D1505 |
| Melt Mass-Flow Rate (MFR) (190°C/21.6 kg) | 21 | g/10 min | ASTM D1238 |
| Environmental Stress-Cracking Resistance (F50) | 200 | hr | ASTM D1693 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 67 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield) | 26.2 | MPa | ASTM D638 |
| Tensile Elongation (Break) | > 600 | % | ASTM D638 |
| Flexural Modulus - 1% Secant | 1000 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Impact Strength | 260 | kJ/m² | ASTM D1822 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (0.45 MPa, Unannealed) | 74.0 | °C | ASTM D648 |
| Brittleness Temperature 1 | < -76.0 | °C | ASTM D746 |
| Vicat Softening Temperature | 126 | °C | ASTM D1525 |
| Note Message | |
|---|---|
| 1 . | F50 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 1387 TFE 10 | RTP Company | PPS | RTP |
| RTP 1405 N L | RTP Company | PESU | RTP |
| Starglas FF001 | Eurostar Engineering Plastics | HDPE | Starglas |
| MOSTEN NB 108 | UNIPETROL RPA | PP Homopolymer | MOSTEN |
| Vi-Chem PVC V221-70E | Vi-Chem Corporation | PVC, Unspecified | Vi-Chem PVC |