Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | Solvay Engineering Plastics |
Trademark: | TECHNYL STAR® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | MqkPg5_TECHNYLSTARS218V35NATURAL.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
TECHNYL STAR® S 218 V35 Natural is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 35% of glass fibre, for injection moulding. Due to its outstanding flow caracteristics, this grade provides a significant productivity improvement and allows more freedom in mould and part design versus a standard polyamide solutions. |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.41 | -- | g/cm³ | ISO 1183/A |
Water Absorption | ISO 62 | |||
23°C, 24 hr | 0.90 | -- | % | ISO 62 |
Equilibrium, 23°C, 50% RH | 1.9 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 11000 | 7400 | MPa | ISO 527-2/1A |
Tensile Stress (Break, 23°C) | 195 | 115 | MPa | ISO 527-2/1A |
Tensile Strain (Break, 23°C) | 3.0 | 4.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 10000 | 6200 | MPa | ISO 178 |
Flexural Stress (23°C) | 285 | 195 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 11 | 16 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | 60 | 70 | kJ/m² | ISO 179/1eU |
Notched Izod Impact (23°C) | 11 | 16 | kJ/m² | ISO 180 |
Unnotched Izod Impact Strength (23°C) | 75 | 80 | kJ/m² | ISO 180/1U |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 210 | -- | °C | ISO 75-2/Af |
Melting Temperature | 222 | -- | °C | ISO 11357-3 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (3.2 mm) | HB | -- | UL 94 | |
Glow Wire Flammability Index (1.6 mm) | 650 | -- | °C | IEC 60695-2-12 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 230 - 235 | °C | |
Middle Temperature | 235 - 240 | °C | |
Front Temperature | 240 - 245 | °C | |
Mold Temperature | 60 - 90 | °C |
Injection instructions |
---|
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
tefabloc® TP SD 333 60A | Mitsubishi Chemical Performance Polymers, Inc. | TPE | tefabloc® |
Varcum 29315 | Durez Corporation | Phenolic | Varcum |
ASTATAL™ F2054 | Marplex Australia Pty. Ltd. | Acetal (POM) Homopolymer | ASTATAL™ |
Ferro PP TPP20AE33BK | Ferro Corporation | PP Homopolymer | Ferro PP |
LNP™ LUBRICOMP™ YL003C compound | SABIC Innovative Plastics | TPEE | LNP™ LUBRICOMP™ |