Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | Taro Plast S.p.A. |
Trademark: | TAROPRENE® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Mho52r_TAROPRENE-1-A25-E1N.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Thermoplastic Elastomer Vulcanized. This TPE-V compound combines the typical performance of a vulcanized elastomer with the easy processing of a thermoplastic compound. Taroprene is totally recyclable and it can be produced in standard grades and in tailor-made grades. Available in natural, black or colored grade. |
General Information | |
---|---|
Features |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.960 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/5.0 kg) | 2.5 | g/10 min | ISO 1133 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore A, 3 sec) | 25 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress 1 | ASTM D412 | ||
100% Strain | 0.500 | MPa | |
300% Strain | 1.11 | MPa | |
Tensile Strength 2(Break) | 2.50 | MPa | ASTM D412 |
Tensile Elongation 3(Break) | 500 | % | ASTM D412 |
Tear Strength | 10.0 | kN/m | ASTM D624 |
Compression Set | ASTM D395B | ||
70°C, 22 hr | 23 | % | |
100°C, 22 hr | 28 | % |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 2.0 | hr | |
Processing (Melt) Temp | 160 to 210 | °C |
Note Message | |
---|---|
1 . | Die C |
2 . | Die C |
3 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Salflex 620KC4 | Salflex Polymers Ltd. | PP, Unspecified | Salflex |
STERLENE™ BMV212 | R&P (Pte.) Ltd. | TPO (POE) | STERLENE™ |
ELASTOSIL® R 701/50 | Wacker Chemie AG | Silicone | ELASTOSIL® R |
KOCETAL® GB706 | Kolon Plastics, Inc. | Acetal (POM) Copolymer | KOCETAL® |
Durethan® C 38 F 000000 | LANXESS GmbH | Nylon 6 | Durethan® |