| Category: | Acetal (POM) Copolymer , Acetal (POM) Copolymer |
| Manufacturer: | YunNan YunTianHua Co., Ltd. |
| Trademark: | YUNTIANHUA® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | McGoeB_YUNTIANHUA-CM90.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
YUNTIANHUA®CM90 is a polyoxymethylene (POM) copolymer product,. It can be processed by extrusion or injection molding and is available in North America, Europe or Asia Pacific. YUNTIANHUA®CM90 applications include engineering/industrial parts and automotive industries. Features include:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.41 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 9.0 | g/10 min | ISO 1133 |
| Water Absorption (23°C, 24 hr) | 0.60 | % | ISO 62 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2700 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 64.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 35 | % | ISO 527-2 |
| Flexural Modulus | 2600 | MPa | ISO 178 |
| Flexural Stress | 88.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | 6.0 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 95.0 | °C | ISO 75-2/A |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 - 90.0 | °C | |
| Drying Time | 3.0 - 4.0 | hr | |
| Rear Temperature | 160 - 180 | °C | |
| Middle Temperature | 170 - 200 | °C | |
| Front Temperature | 190 - 210 | °C | |
| Nozzle Temperature | 180 - 210 | °C | |
| Processing (Melt) Temp | 180 - 210 | °C | |
| Mold Temperature | 60.0 - 90.0 | °C | |
| Injection Pressure | 50.0 - 100 | MPa | |
| Holding Pressure | 30.0 - 80.0 | MPa | |
| Back Pressure | 0.00 - 0.500 | MPa | |
| Screw Speed | 50 - 120 | rpm |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Melt Temperature | 180 - 190 | °C |
| Extrusion instructions |
|---|
| Standard extruders with grooved feed zone and short compression screws (minimum 25 D) will fit. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP ESD C 280 | RTP Company | Nylon 66 | RTP |
| Royalene® 580HT | Lion Copolymer, LLC | EPDM | Royalene® |
| Sinpolene GPP1630 | Teknor Apex Asia Pacific PTE. LTD. | PP Homopolymer | Sinpolene |
| Boda BDF-KK2702 | Chenguang Fluoro & Silicone Elastomers Co., Ltd. | Fluorelastomer | Boda |
| Luran® S KR2858G3 | Styrolution | ASA | Luran® S |