| Category: | PVC, Unspecified , Polyvinyl Chloride |
| Manufacturer: | Sylvin Technologies Incorporated |
| Trademark: | Sylvin |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | MZzTvu_Sylvin826075Grey9595.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Sylvin 8260-75 Grey 9595 Is A Vinyl Compound Formulated For Electrical Molding Applications. |
| General Information | |
|---|---|
| Uses |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.40 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shaw A | 75 | ASTM D2240 | |
| Shaw A, 10 seconds | 75 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 12.1 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 330 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength | 50.8 | kN/m | ASTM D624 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | -32.0 | °C | ASTM D746 |
| Melting Temperature | 163 - 174 | °C |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Oxygen Index | 23 | % | ASTM D2863 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| MTEGRITY™ PP Impact Copolymer CP410 | M. Holland Company | PP Impact Copolymer | MTEGRITY™ PP Impact Copolymer |
| VESTAMID® D DX9321 | Evonik Industries AG | Nylon 612 | VESTAMID® D |
| Kumho SBR 1778K | Korea Kumho Petrochemical Co., Ltd. | SBR, Emulsion | Kumho SBR |
| Innothane® IE-60AC | Innovative Polymers, Inc. | TSU-Ester | Innothane® |
| PENTAMID B GK30 H LS natural | PENTAC Polymer GmbH | Nylon 6 | PENTAMID B |