| Category: | PP Homopolymer , Polypropylene Homopolymer |
| Manufacturer: | Osterman & Company |
| Trademark: | Osterlene® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | MP4q8u_OsterlenePPH20NA.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Uses |
|
| Agency Ratings |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 20 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Rockwell Hardness (R-Scale) | 108 | ASTM D785 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Yield) | 25.5 | MPa | ASTM D638 |
| Tensile Elongation (Yield) | 20 | % | ASTM D638 |
| Flexural Modulus | 896 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 48 | J/m | ASTM D256 |
| Dart Drop Impact | 1.39 | J | ASTM D5420 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (0.45 MPa, Unannealed) | 106 | °C | ASTM D648 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SANREX S10G20 | Techno Polymer Co, Ltd. | SAN | SANREX |
| SAXAMID™ 136F6Q32 | SAX Polymers | Nylon 6 | SAXAMID™ |
| Sofprene T® 540200A60 | SO.F.TER. SPA | SBS | Sofprene T® |
| Edgetek鈩?AT-20GF/000 BLACK | PolyOne Corporation | Acetal (POM) Copolymer | Edgetek™ |
| Sylvin 7833-75 Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |