Category: | Nylon 6 , Polyamide 6 |
Manufacturer: | EMS-GRIVORY |
Trademark: | Grilon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | LKgAOs_Grilon-EBV-15H-Black-9697.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Grilon® EBV-15H Black 9697 is a Polyamide 6 (Nylon 6) material filled with 15% glass fiber. It is available in Asia Pacific, Europe, or North America for blow molding or extrusion. Important attributes of Grilon® EBV-15H Black 9697 are:
Typical applications include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Uses |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.21 | -- | g/cm³ | ISO 1183 |
Water Absorption | ISO 62 | |||
Saturation, 23°C | 8.0 | -- | % | |
Equilibrium, 23°C, 50% RH | 2.5 | -- | % |
Hardness | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Ball Indentation Hardness | 145 | 70.0 | MPa | ISO 2039-1 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus | 5600 | 2700 | MPa | ISO 527-2 |
Tensile Stress (Break) | 110 | 65.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 5.0 | 25 | % | ISO 527-2 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | |||
-30°C | 6.0 | 8.0 | kJ/m² | |
23°C | 15 | 30 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179/1eU | |||
-30°C | 80 | 80 | kJ/m² | |
23°C | 80 kJ/m² | No Break |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature | ||||
1.8 MPa, Unannealed | 165 | -- | °C | ISO 75-2/A |
8.0 MPa, Unannealed | 50.0 | -- | °C | ISO 75-2/C |
Maximum Use Temperature | Internal Method | |||
Long Term | 100 to 120 | -- | °C | |
Short Term | 180 | -- | °C |
Additional Information | Dry | Conditioned | Test Method | |
---|---|---|---|---|
ISO Type | PA 6-HI, BH, 27-060, GF15 | -- | ISO 1874 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Melting Temperature 1 | 222 | -- | °C | ISO 11357-3 |
CLTE | ISO 11359-2 | |||
Flow | 5.0E-5 | -- | cm/cm/°C | |
Transverse | 1.2E-4 | -- | cm/cm/°C |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | -- | 1.0E+10 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+13 | 1.0E+11 | ohms·cm | IEC 60093 |
Electric Strength | 26 | 22 | kV/mm | IEC 60243-1 |
Comparative Tracking Index | -- | 325 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flammability Classification (0.800 mm) | HB | -- | IEC 60695-11-10, -20 |
Note Message | |
---|---|
1 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Salflex 262EI | Salflex Polymers Ltd. | TPO (POE) | Salflex |
XANTAR® C CM 506 U | Mitsubishi Engineering-Plastics Corp | PC+ABS | XANTAR® C |
Xuchuan XCD-45DC | Xuchuan Chemical (Suzhou) Co., Ltd | PUR, Unspecified | Xuchuan |
Cevian®-V VF191 | Daicel Polymer Ltd. | ABS | Cevian®-V |
Sumiliteresin® PR-50869 BI | SBHPP | Phenolic | Sumiliteresin® |