| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | A. Schulman Europe |
| Trademark: | SCHULAMID® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Ky6gp5_SCHULAMID-66-GF-15-HI-K2034.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 15% glass fiber reinforced, impact modified polyamide 66 compound |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Processing Method |
|
| Resin ID (ISO 1043) |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.21 | -- | g/cm³ | ISO 1183/A |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 5400 | 3000 | MPa | ISO 527-2/1A/1 |
| Tensile Stress (Break) | 100 | 60.0 | MPa | ISO 527-2/1A/5 |
| Tensile Strain (Break) | 4.0 | 18 | % | ISO 527-2/1A/5 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ||||
| -30°C | 3.5 | -- | kJ/m² | ISO 179 |
| 23°C | 12 | 24 | kJ/m² | ISO 179/1eA |
| Charpy Unnotched Impact Strength | ||||
| -30°C | 40 | -- | kJ/m² | ISO 179 |
| 23°C | 60 kJ/m² | No Break | ISO 179/1eU |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature | ||||
| 0.45 MPa, Unannealed | 240 | -- | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 215 | -- | °C | ISO 75-2/A |
| Vicat Softening Temperature | ||||
| -- | > 250 | -- | °C | ISO 306/A50 |
| -- | 225 | -- | °C | ISO 306/B50 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Stylac™ A4130 | Asahi Kasei Chemicals Corporation | ABS | Stylac™ |
| STYRON™ C-TECH HIPS | Trinseo | PS (HIPS) | STYRON™ C-TECH |
| ALAMID® 6 GF 25 HV SCHWARZ-9957 | LEIS Polytechnik - polymere Werkstoffe GmbH | Nylon 6 | ALAMID® |
| Delta N6-2400 | Delta Polymers | Nylon 6 | Delta |
| LNP™ THERMOCOMP™ ECF62 compound | SABIC Innovative Plastics | PEI | LNP™ THERMOCOMP™ |