Category: | MDPE , Medium Density Polyethylene |
Manufacturer: | Borealis AG |
Trademark: | Borealis PE |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | KupBmt_Borealis-PE-ME6032.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
It is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications ME6032 is intended for Dry core and petroleum jelly filled cables Specifications ME6032 meets the following material classification:
Cables manufactured with ME6032 using sound extrusion practice normally comply with the following cable product standards: IEC 60708 IEC 61156 EN 50288 EN 50407 |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.928 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 0.30 | g/10 min | ISO 1133 |
Environmental Stress-Cracking Resistance (50°C, 100% Igepal, F20) | > 250 | hr |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D, 1 sec) | 53 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield) | 17.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 600 | % | ISO 527-2 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | < -76.0 | °C | ASTM D746 |
Oxidation Induction Time (200°C) | 50 | min | IEC 60811-4-2/B |
Additional Information | Nominal Value | Unit | Test Method |
---|---|---|---|
Petroleum jelly absorption | 8.0 | % | IEC 60811-4-2 |
Resistance to Thermal Ageing (105°C) | > 1.4 | month | IEC 60811-4-2/A |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | 1.0E+16 | ohms·cm | IEC 60093 |
Dielectric Strength | 22 | kV/mm | IEC 60243-1 |
Dielectric Constant (1 MHz) | 2.30 | IEC 60250 | |
Dissipation Factor (1 MHz) | 1.5E-4 | IEC 60250 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 165 - 230 | °C | |
Cylinder Zone 2 Temp. | 165 - 230 | °C | |
Cylinder Zone 3 Temp. | 165 - 230 | °C | |
Cylinder Zone 4 Temp. | 165 - 230 | °C | |
Melt Temperature | 220 - 240 | °C | |
Die Temperature | 230 | °C |
Extrusion instructions |
---|
Conductor preheating temperature: 70 to 100 °C - 2400 m/minLine speed |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sinvicomp SRP3605A | Teknor Apex Asia Pacific PTE. LTD. | PVC, Rigid | Sinvicomp |
4MID® 9B22115 HFR1 | 4Plas | Nylon 6 | 4MID® |
Kingfa JH710 G15 | Kingfa | PC Alloy | Kingfa |
LNP™ LUBRICOMP™ IBP34 compound | SABIC Innovative Plastics | Nylon 612 | LNP™ LUBRICOMP™ |
Osterlene® GPPS1400 | Osterman & Company | PS (GPPS) | Osterlene® |