| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Ravago Group |
| Trademark: | Ravamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | KCw4Dz_Ravamid-R210-MGF-5-25.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 30% Glass fibre and mineral reinforced PA6.6 compound for injection moulding |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.36 | g/cm³ | ISO 2781 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 1.4 | % | |
| Flow | 0.50 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 7800 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 145 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 2.8 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength | 7.0 | kJ/m² | ISO 180/1A |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 256 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 252 | °C | ISO 306/A120 |
| Melting Temperature | 260 to 265 | °C |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating 1(1.60 mm) | HB | Internal Method |
| Note Message | |
|---|---|
| 1 . | UL94 internally tested |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| STARFLEX® P 7393-1000 | STAR Thermoplastic Alloys & Rubbers, Inc. | TPE | STARFLEX® |
| WELLAMID Nylon 6600 PA-66-HWL | CP-Polymer-Technik GmbH & Co. KG | Nylon 66 | WELLAMID Nylon |
| Badadur® PBT8 GF30 TM-Z2 | Bada AG | PBT | Badadur® |
| Elastollan® L 785 A | BASF Polyurethanes GmbH | TPU-Polyester | Elastollan® |
| Plaslube® PC / ABS 1110 | Techmer Engineered Solutions | PC+ABS | Plaslube® |