Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Teknor Apex Company |
Trademark: | Sarlink® TPE |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | In6Wze_Sarlink-TPE-RV-1675DN-XRD.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Sarlink®TPE RV-1675DN XRD is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding. Sarlink®The main characteristics of TPE RV-1675DN XRD are: high hardness. Typical application areas include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.05 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 10 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shore D, 1 second, injection molding | 76 | ASTM D2240 | |
Shore D, 5 seconds, injection molding | 75 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Break) | 31.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 200 | % | ASTM D412 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Rear Temperature | 171 - 193 | °C | |
Middle Temperature | 177 - 199 | °C | |
Front Temperature | 182 - 204 | °C | |
Nozzle Temperature | 188 - 210 | °C | |
Processing (Melt) Temp | 188 - 210 | °C | |
Mold Temperature | 25.0 - 65.6 | °C | |
Injection Pressure | 1.38 - 6.89 | MPa | |
Injection Rate | Moderate-Fast | ||
Back Pressure | 0.172 - 0.345 | MPa | |
Screw Speed | 50 - 100 | rpm | |
Cushion | 3.81 - 25.4 | mm |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 166 - 188 | °C | |
Cylinder Zone 2 Temp. | 171 - 193 | °C | |
Cylinder Zone 3 Temp. | 177 - 199 | °C | |
Cylinder Zone 5 Temp. | 182 - 204 | °C | |
Die Temperature | 190 - 210 | °C |
Extrusion instructions |
---|
Screw Speed: 30 to 100 rpm |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PrimoPrene 45D-1000 | KMI Group Inc. | TPV | PrimoPrene |
SLOVASTER® C FRU 2 | Plastcom | PC | SLOVASTER® |
Daelim Po1y® PH-780B | DAELIM INDUSTRIAL CO., LTD. | PP Homopolymer | Daelim Po1y® |
Fainplast PVC RE 220 | Fainplast Compounds S.r.l | PVC, Rigid | Fainplast PVC |
POCAN® TP 306-201 000000 | LANXESS GmbH | PBT+ASA | POCAN® |