Category: | LDPE , Low Density Polyethylene |
Manufacturer: | Celanese EVA Performance Polymers |
Trademark: | AT |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | I3z5rg_AT-520.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
AT 520 is an LDPE product recommended for general film resin. |
General Information | |
---|---|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.921 | g/cm³ | ASTM D1505 |
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg) | 2.0 | g/10 min | ASTM D1238 |
Films | Nominal Value | Unit | Test Method |
---|---|---|---|
Film Thickness - Tested | 50 | µm | |
Secant Modulus | ASTM D882 | ||
1% Secant, MD : 50 µm, Blown Film | 210 | MPa | |
1% Secant, TD : 50 µm, Blown Film | 240 | MPa | |
Tensile Strength 1 | ASTM D882 | ||
MD : Yield, 50 µm, Blown Film | 12.0 | MPa | |
TD : Yield, 50 µm, Blown Film | 12.0 | MPa | |
MD : Break, 50 µm, Blown Film | 21.0 | MPa | |
TD : Break, 50 µm, Blown Film | 20.0 | MPa | |
Tensile Elongation 2 | ASTM D882 | ||
MD : Break, 50 µm, Blown Film | 400 | % | |
TD : Break, 50 µm, Blown Film | 600 | % | |
Dart Drop Impact (50 µm, Blown Film) | 100 | g | ASTM D1709 |
Optical | Nominal Value | Unit | Test Method |
---|---|---|---|
Gloss (45°, 50.0 µm, Blown Film) | 54 | ASTM D2457 | |
Haze (50.0 µm, Blown Film) | 14 | % | ASTM D1003 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 170 to 230 | °C |
Note Message | |
---|---|
1 . | 500 mm/min |
2 . | 500 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
VESTOLIT® E 6007 | VESTOLIT GmbH & Co. KG | PVC, Unspecified | VESTOLIT® |
4LEX® 9F22110 FR1 | 4Plas | PC | 4LEX® |
ARMAMID® PA 6-3EK | Poly Plastic | Nylon 6 | ARMAMID® |
KYOCERA KE-200DH | KYOCERA Chemical Corporation | Epoxy | KYOCERA |
Sylvin 7844-65 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |