Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.15 to 1.25 | g/cm³ | ISO 1183 |
Molding Shrinkage | 1.0 to 1.1 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore D) | 75 to 80 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 1400 to 2800 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 40.0 to 70.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | > 15 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength | > 6.0 | kJ/m² | ISO 180/1A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 85.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | 215 | °C | ISO 306/B |
Melting Temperature (DSC) | 220 | °C | ISO 3146 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | V-0 | UL 94 | |
Glow Wire Ignition Temperature | 960 | °C | VDE 0471/2 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Precision Polymer A95H | Precision Polymer Engineering Ltd. | Rubber | Precision Polymer |
Styrolution PS 168N | INEOS Styrolution Group GmbH | PS (GPPS) | Styrolution PS |
Amodel® AT-1125 HS | Solvay Specialty Polymers | PPA | Amodel® |
WELLAMID Nylon 6600/42 GS 30 HWCP | CP-Polymer-Technik GmbH & Co. KG | Nylon 66 | WELLAMID Nylon |
SCLAIR® 2807CC-NS | NOVA Chemicals | HDPE | SCLAIR® |