Category: | PP Copolymer , Polypropylene Copolymer |
Manufacturer: | EMAS Plastik San.Tic.AS. |
Trademark: | EMOPLEN® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | HFTGEn_EMOPLEN-CP-MTF-10.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Polypropylene copolymer %10 talcum filled |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.900 to 1.00 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 3.0 to 20 | g/10 min | ISO 1133 |
Molding Shrinkage | 0.95 to 1.1 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness (Shore D) | 60 to 65 | ISO 868 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 2000 to 3000 | MPa | ISO 527-2 |
Tensile Stress (Yield) | 20.0 to 35.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | > 15 | % | ISO 527-2 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength | > 6.0 | kJ/m² | ISO 180/1A |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 100 | °C | ISO 75-2/A |
Vicat Softening Temperature | 95.0 | °C | ISO 306/B |
Melting Temperature (DSC) | 160 | °C | ISO 3146 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SWANCOR Epoxy 901-35 | SWANCOR IND. CO., LTD. | Epoxy | SWANCOR Epoxy |
TAROLOX 2050 W G6 | Taro Plast S.p.A. | PBT+PET | TAROLOX |
Tarnoform® 300 WD | Grupa Azoty S.A. | Acetal (POM) Copolymer | Tarnoform® |
Celanex® 2300 GV1/20 | Celanese Corporation | PBT | Celanex® |
Laprene® 83E200A75 | SO.F.TER. SPA | SEBS | Laprene® |