| Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
| Manufacturer: | COIM S.p.A. |
| Trademark: | LARIPUR® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | H4OF3d_LARIPUR-LPR-9060EM.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
LARIPUR®LPR 9060EM is a thermoplastic polyurethane elastomer (polyether)(TPU-polyether) material,. This product is available in North America, Latin America or Europe. The processing method is: extrusion or injection molding. LARIPUR®The main features of LPR 9060EM are:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.10 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 88 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ASTM D412 | ||
| 50% strain | 5.80 | MPa | ASTM D412 |
| 100% strain | 7.50 | MPa | ASTM D412 |
| 300% strain | 13.5 | MPa | ASTM D412 |
| Tensile Strength (Break) | 44.2 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 590 | % | ASTM D412 |
| Tear Strength | 81.0 | kN/m | ASTM D624 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating | V-2 | UL 94 |
| Additional Information |
|---|
| Abrasion loss, DIN 53516: 30 mm³ |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP VLF 80207 EM HS | RTP Company | Nylon 66 | RTP |
| SABIC® LDPE 2008N0 | Saudi Basic Industries Corporation (SABIC) | LDPE | SABIC® LDPE |
| Santoprene™ 8211-55 | ExxonMobil Chemical | TPV | Santoprene™ |
| KumhoSunny PET HEG3645 | Shanghai KumhoSunny Plastics Co., Ltd. | PET | KumhoSunny PET |
| Lucet® MR-320 | LG Chem Ltd. | Acetal (POM) Copolymer | Lucet® |