| Category: | PP, Unspecified , Polypropylene |
| Manufacturer: | AD majoris |
| Trademark: | MAJORIS |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | H1AfvG_MAJORIS-CFR280---8487.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
MAJORIS CFR280-8487 is a polypropylene product,. It can be processed by injection molding and is available in Europe. Features include:
|
| General Information | |
|---|---|
| Features |
|
| RoHS Compliance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.38 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 5.0 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flexural Modulus | 2400 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 15 | kJ/m² | ISO 179/1eA |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (1.60 mm) | V-0 | UL 94 | |
| Glow Wire Flammability Index (1.00 mm) | 960 | °C | IEC 60695-2-12 |
| Oxygen Index | 27 | % | ISO 4589-2 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Drying Time | 3.0 | hr | |
| Processing (Melt) Temp | 210 - 240 | °C | |
| Mold Temperature | 30.0 - 50.0 | °C | |
| Injection Rate | Moderate |
| Injection instructions |
|---|
| Holding pressure: 50 to 70% of the injection pressure |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 1207-75A | RTP Company | TPU-Polyester | RTP |
| RTP 103 FR UV | RTP Company | PP, Unspecified | RTP |
| Mylar® D1 (700 guage) | DuPont Teijin Films U.S. | PET | Mylar® |
| Elastron® G G103.A80.N | Elastron USA, Inc. | SEBS | Elastron® G |
| Sylvin 9067-90 GREY 9193 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |