It is a soft, colorable, UV-resistant thermoplastic vulcanized elastomer (TPV) in the thermoplastic elastomer (TPE) series. This material has good physical properties and chemical resistance at the same time, and is suitable for a wide range of fields. This brand of Shanduping TPV is a shear rate dependent product that can be processed on conventional thermoplastic injection molding or blow molding equipment. This is a polyolefin-based material that can be recycled in the production process.
General Information
Features
  • Good dimensional stability
  • Low friction coefficient
  • Low hygroscopicity
  • Good UV resistance
  • Recyclable materials
  • Good color stability
  • Good coloring
  • Ozone resistance
  • Good chemical resistance
  • Good weather resistance
  • Low or no water absorption
  • Medium hardness
Uses
  • Architectural application field
  • Expansion Joint
  • Outdoor application
  • Assembled glass
Agency Ratings
  • UL QMFZ2
  • UL QMFZ8
RoHS Compliance
  • RoHS compliance
UL File Number
  • E80017
Appearance
  • Natural color
Forms
  • Particle
Processing Method
  • Blow molding
  • Multiple injection molding
  • Extrusion blow molding
  • Injection blowing molding
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity
    -- 0.948g/cm³ASTM D792
    -- 0.950g/cm³ISO 1183
Outdoor Suitability f1UL 746C
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shaw A, 15 seconds, 23°C, 2.00mm)75ISO 868
ElastomersNominal ValueUnitTest Method
Tensile Stress - Across Flow (100% Strain, 23°C)2.90MPaASTM D412, ISO 37
Tensile Strength - Across Flow (Break, 23°C)6.80MPaASTM D412, ISO 37
Tensile Elongation - Across Flow (Break, 23°C)600%ASTM D412, ISO 37
Tear Strength - Across Flow
    23°C 125.0kN/mASTM D624
    23°C 225kN/mISO 34-1
Compression Set
    70°C, 22 hr 338%ASTM D395B
    125°C, 70 hr 458%ASTM D395B
    70°C, 22 hr 538%ISO 815
    125°C, 70 hr 658%ISO 815
ThermalNominal ValueUnitTest Method
Brittleness Temperature -62.0°CASTM D746, ISO 812
RTI Elec 100°CUL 746
RTI 85.0°CUL 746
ElectricalNominal ValueTest Method
Comparative Tracking Index (CTI) PLC 0UL 746
High Amp Arc Ignition (HAI) PLC 1UL 746
FlammabilityNominal ValueTest Method
Flame Rating UL 94
    1.10 mm HBUL 94
    1.60 mm HBUL 94
    3.00 mm HBUL 94
Additional Information
如果适用,这是基于扇形浇口注塑成型的平板测试结果。拉伸强度、伸长率和拉伸应力沿垂直流动方向测定 - ISO 1 型,ASTM die C。25% 形变时的永久压缩变形。从埃克森美孚欧洲分支机构直接购买的所有产品都符合 REACH 法规。 对于埃克森 美孚未进口至欧洲的产品,用户应自行评估其是否满足 REACH 法规。
Legal statement
未经埃克森美孚化工书面允许,这种产品包括其产品名称,不得在任何医疗应用领域予以使用或有关详细的产品监管信息,请联系客户服务。
InjectionNominal ValueUnit
Drying Temperature 82.2°C
Drying Time 3.0hr
Suggested Max Moisture 0.080%
Suggested Max Regrind 20%
Rear Temperature 179 - 196°C
Middle Temperature 185 - 199°C
Front Temperature 191 - 204°C
Nozzle Temperature 191 - 210°C
Processing (Melt) Temp 199 - 216°C
Mold Temperature 23.9 - 51.7°C
Injection Rate Fast
Back Pressure 0.345 - 0.689MPa
Screw Speed 100 - 200rpm
Clamp Tonnage 4.1 - 6.9kN/cm²
Cushion 3.18 - 6.35mm
Screw L/D Ratio 16.0:1.0 to 20.0:1.0
Screw Compression Ratio 2.0:1.0 to 2.5:1.0
Vent Depth 0.025mm
Injection instructions
Santoprene TPV与乙缩醛和PVC不相容。更多关于加工和模具设计的信息,请查阅我们的《注射成型指南》。
ExtrusionNominal ValueUnit
Melt Temperature 185 - 221°C
Die Temperature 185 - 221°C
Note Message
1 .C mould
2 .Method B, right-angle specimen (cut)
3 .Type 1
4 .Type 1
5 .Type a
6 .Type a
Resin Grade Manufacturer Category Trademark
Monprene® RG-10170 X (PRELIMINARY DATA) Teknor Apex Company TPE Monprene®
Baoding 67I70 Baoding Bangtai Polymeric New-Materials Co.,Ltd TPU-Polyester Baoding
Ferro PP TPP40AJ32BK Ferro Corporation PP Homopolymer Ferro PP
Lupox® GP2306FS LG Chem Ltd. PBT Lupox®
Plasmer 1075B/8901 HYUNDAI EP Co., Ltd. TPE Plasmer