| Category: | PP Homopolymer , Polypropylene Homopolymer |
| Manufacturer: | Polykemi AB |
| Trademark: | POLYfill |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | GuSUPk_POLYfill-PPH-GF5040-PD2.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass fibre-reinforced Chemically coupled |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.22 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 5.0 | g/10 min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 95.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 3.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 7600 | MPa | ISO 178 |
| Flexural Stress | 140 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -20°C | 6.0 | kJ/m² | |
| 23°C | 8.0 | kJ/m² |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1 | |||
| 0.45 MPa, Unannealed | 160 | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 153 | °C | ISO 75-2/A |
| Vicat Softening Temperature | 166 | °C | ISO 306/A50 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (1.60 mm) | HB | UL 94 | |
| Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 4099 X 131005 B | RTP Company | PPA | RTP |
| Badadur® PBT/PC FR V0 | Bada AG | PC+PBT | Badadur® |
| HiFill® PA6/6 GF33 UV BK001 | Techmer Engineered Solutions | Nylon 66/6 | HiFill® |
| Hipolyene 1532 HC EX | Zylog Plastalloys | TPO (POE) | Hipolyene |
| Idemitsu PS SEHI-102 | Idemitsu PS | PS (HIPS) | Idemitsu PS |