| Category: | Acetal (POM) Copolymer , Acetal (POM) Copolymer |
| Manufacturer: | KEP Americas |
| Trademark: | Kepital® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | GeYmK4_Kepital-F20-03-LOF.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Low emission, standard medium viscosity grade |
| General Information | |
|---|---|
| Features |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.41 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) | 9.0 | g/10 min | ISO 1133 |
| Molding Shrinkage - Flow (3.00 mm) | 2.0 | % | ISO 294-4 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Break, 23°C) | 64.0 | MPa | ISO 527-2 |
| Nominal Tensile Strain at Break (23°C) | 37 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 2500 | MPa | ISO 178 |
| Flexural Stress (23°C) | 87.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | 6.5 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 100 | °C | ISO 75-2/A |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | 1.0E+16 | ohms | IEC 60093 |
| Volume Resistivity | 1.0E+14 | ohms·cm | IEC 60093 |
| Electric Strength | 19 | kV/mm | IEC 60243-1 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating | HB | UL 94 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 4089 | RTP Company | PPA | RTP |
| Surlyn® 8020 | DuPont Packaging & Industrial Polymers | EMAA | Surlyn® |
| Westlake LDPE EF378 | Westlake Chemical Corporation | LDPE | Westlake LDPE |
| CYCOLOY™ RCX7233 resin | SABIC Innovative Plastics Asia Pacific | PC+ABS | CYCOLOY™ |
| Plaslube® POM CO GF5 TL5 | Techmer Engineered Solutions | Acetal (POM) Copolymer | Plaslube® |