Category: | TPC-ET , THERMOPLASTIC POLYESTER ELASTOMER |
Manufacturer: | DuPont Performance Polymers |
Trademark: | Hytrel® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | GNtMwL_Hytrel-7246HS-NC010.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Part Marking Code (ISO 11469) |
|
Resin ID (ISO 1043) |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.25 | g/cm³ | ISO 1183 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness | ISO 868 | ||
Shore D | 70 | ||
Shore D, 15 sec | 66 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 430 | MPa | ISO 527-2 |
Tensile Stress | ISO 527-2 | ||
Yield | 29.0 | MPa | |
Break | 52.0 | MPa | |
10% Strain | 23.0 | MPa | |
50% Strain | 24.0 | MPa | |
Tensile Strain | ISO 527-2 | ||
Yield | 22 | % | |
Break | > 300 | % | |
Nominal Tensile Strain at Break | 560 | % | ISO 527-2 |
Flexural Modulus | 500 | MPa | ISO 178 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength | ISO 34-1 | ||
Across Flow | 170 | kN/m | |
Flow | 180 | kN/m |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -65.0 | °C | ISO 974 |
Melting Temperature 1 | 216 | °C | ISO 11357-3 |
Note Message | |
---|---|
1 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 4005 FR A HS | RTP Company | PPA | RTP |
RTP 385 TFE 15 FR | RTP Company | PC | RTP |
NORYL™ GFN2 resin | SABIC Innovative Plastics | PPE+PS | NORYL™ |
Chemlon® 225 G | Teknor Apex Company (Chem Polymer) | Nylon 6 | Chemlon® |
Desmoderm® KB2W | Covestro - PUR | PUR-Ester | Desmoderm® |