| Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
| Manufacturer: | BASF Polyurethanes GmbH |
| Trademark: | Elastollan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | GMDSlK_Elastollan-Soft-45-A-ESD.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Thermoplastic Polyester-Polyurethane with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance, plasticized, containing antistatic Additive Processable by injection moulding |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.18 | g/cm³ | ISO 1183/A |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore A) | 47 | ISO 7619 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Abrasion Loss | 60.0 | mm³ | ISO 4649-A |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield) | 30.0 | MPa | ISO 37 |
| Tensile Elongation (Break) | 900 | % | ISO 37 |
| Tear Strength 1 | 35 | kN/m | ISO 34-1 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 5.0E+7 | ohms·cm | IEC 60093 |
| Note Message | |
|---|---|
| 1 . | Method Bb, Angle (Nicked) |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Maxelast® C49C15 | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
| Tislamid® PA66 PA66 50 GFR | Tisan | Nylon 66 | Tislamid® PA66 |
| XYRON™ L544V | Asahi Kasei Chemicals Corporation | PPE+PS | XYRON™ |
| KEP® 650 | Kumho Polychem Co., Ltd. | EPDM | KEP® |
| Leona™ 13G25 | Asahi Kasei Chemicals Corporation | Nylon 66 | Leona™ |