Category: | TPC-ET , THERMOPLASTIC POLYESTER ELASTOMER |
Manufacturer: | DuPont Performance Polymers |
Trademark: | Hytrel® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | GGqRmH_Hytrel-7246HS-BK320.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection |
General Information | |
---|---|
Additive |
|
Features |
|
Uses |
|
Processing Method |
|
Multi-Point Data |
|
Part Marking Code (ISO 11469) |
|
Resin ID (ISO 1043) |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.25 | g/cm³ | ISO 1183 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Shore Hardness | ISO 868 | ||
Shore D | 70 | ||
Shore D, 15 sec | 66 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 480 | MPa | ISO 527-2 |
Tensile Stress | ISO 527-2 | ||
Break | 53.0 | MPa | |
10% Strain | 23.0 | MPa | |
50% Strain | 24.0 | MPa | |
Tensile Strain (Break) | > 300 | % | ISO 527-2 |
Nominal Tensile Strain at Break | 560 | % | ISO 527-2 |
Flexural Modulus | 515 | MPa | ISO 178 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength | ISO 34-1 | ||
Across Flow | 170 | kN/m | |
Flow | 180 | kN/m |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -70.0 | °C | ISO 974 |
Melting Temperature 1 | 216 | °C | ISO 11357-3 |
Note Message | |
---|---|
1 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Radilon® S ERV2510 100 NAT | Radici Plastics | Nylon 6 | Radilon® |
Telcar® TL-1996E NAT | Teknor Apex Company | TPE | Telcar® |
LEXAN™ 505RU resin | SABIC Innovative Plastics | PC | LEXAN™ |
ESTOPLAST EP 1500BB01 | Ester Industries Ltd. | PBT | ESTOPLAST EP |
Pro-fax SB912 | LyondellBasell Industries | PP Copolymer | Pro-fax |