TECHNYL® C 230 Natural is an unreinforced polyamide 6, with improved impact resistance, for injection moulding. This grade offers improved impact strength and higher flexibility. The grade is designed to make technical parts having small or medium sizeThis product is available in natural color. |
General Information | |
---|---|
Additive |
|
Features |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Resin ID (ISO 1043) |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1.14 | -- | g/cm³ | ISO 1183/A |
Water Absorption | ISO 62 | |||
23°C, 24 hr | 1.2 | -- | % | ISO 62 |
Saturated, 23°C | 9.0 | -- | % | ISO 62 |
Equilibrium, 23°C, 50% RH | 3.3 | -- | % | ISO 62 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile Modulus (23°C) | 2600 | 720 | MPa | ISO 527-2/1A |
Tensile Stress | ISO 527-2/1A | |||
Yield, 23°C | 65.0 | 30.0 | MPa | ISO 527-2/1A |
Fracture, 23°C | 45.0 | 35.0 | MPa | ISO 527-2/1A |
Tensile Strain | ISO 527-2 | |||
Yield, 23°C | 7.0 | 30 | % | ISO 527-2 |
Fracture, 23°C | > 50 | > 200 | % | ISO 527-2 |
Flexural Modulus (23°C) | 2500 | 800 | MPa | ISO 178 |
Flexural Stress (23°C) | 100 | 35.0 | MPa | ISO 178 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy Notched Impact Strength (23°C) | 11 | 90 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C) | No Break | No Break | ISO 179/1eU | |
Notched Izod Impact (23°C) | 9.0 | 80 | kJ/m² | ISO 180 |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 75.0 | -- | °C | ISO 75-2/Af |
Melting Temperature | 222 | -- | °C | ISO 11357-3 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface Resistivity | 1.0E+14 | 1.0E+12 | ohms | IEC 60093 |
Volume Resistivity | 1.0E+15 | 1.0E+13 | ohms·cm | IEC 60093 |
Dielectric Strength (2.00 mm) | -- | 18 | kV/mm | IEC 60243-1 |
Relative Permittivity | 3.50 | 4.00 | IEC 60250 | |
Dissipation Factor | 0.20 | 0.12 | IEC 60250 | |
Comparative Tracking Index (Solution A) | 600 | 600 | V | IEC 60112 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Flame Rating (1.6 mm) | HB | -- | UL 94 |
Injection | Dry | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Suggested Max Moisture | 0.20 | % | |
Rear Temperature | 230 - 235 | °C | |
Middle Temperature | 235 - 240 | °C | |
Front Temperature | 235 - 245 | °C | |
Mold Temperature | 60 - 80 | °C |
Injection instructions |
---|
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For unfilled polyamide, Solvay recommends the use of high alloy steel with a weak chromium content. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
ProvaMed® TPE 1070 | ACTEGA GmbH | TPE | ProvaMed® TPE |
Tisester® PBT 30 GFR FR | Tisan | PBT | Tisester® |
Cytec BPS240 format 2 | Cytec Industries Inc. | Epoxy | Cytec |
Luxus PP 16194 | Luxus Limited | PP, Unspecified | Luxus PP |
Plaslube® POM HO TL20 BK | Techmer Engineered Solutions | Acetal (POM) Homopolymer | Plaslube® |