| Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
| Manufacturer: | BASF Polyurethanes GmbH |
| Trademark: | Elastollan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Fq0pAb_Elastollan-1160-D.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms. Typical applications Cable jackets, plugs and terminations, spiral tubing, Films, ski-boot shells, ear tags, technical mouldings like mining screens, railway pads, seals. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.18 | g/cm³ | ISO 1183/A |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D, 3 sec) | 60 | ISO 7619 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 200 | MPa | ISO 527-2 |
| Abrasion Loss | 20.0 | mm³ | ISO 4649-A |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | DIN 53504 | ||
| 20% Strain | 13.0 | MPa | |
| 100% Strain | 19.0 | MPa | |
| 300% Strain | 41.0 | MPa | |
| Tensile Stress | DIN 53504 | ||
| Yield 1 | 35.0 | MPa | |
| Yield | 50.0 | MPa | |
| Tensile Elongation | DIN 53504 | ||
| Break 2 | 450 | % | |
| Break | 400 | % | |
| Tear Strength 3 | 170 | kN/m | ISO 34-1 |
| Compression Set | ISO 815 | ||
| 23°C, 72 hr | 40 | % | |
| 70°C, 24 hr | 50 | % |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | ||
| -30°C | 16 | kJ/m² | |
| 23°C | No Break |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Processing (Melt) Temp | 170 to 240 | °C | |
| Mold Temperature | 20.0 to 70.0 | °C |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Melt Temperature | 160 to 220 | °C |
| Note Message | |
|---|---|
| 1 . | after storage in water at 80°C for 42 days |
| 2 . | after storage in water at 80°C for 42 days |
| 3 . | Method Bb, Angle (Nicked) |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Tecnoprene® VK10 NERO900 | SO.F.TER. SPA | PP Homopolymer | Tecnoprene® |
| Cawiton® CN930 | Wittenburg B.V. | SEBS | Cawiton® |
| ELASTOSIL® R plus 4370/50 | Wacker Chemie AG | Silicone | ELASTOSIL® R plus |
| Sylvin 8663-65 Clear | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
| ULTEM™ 9090 resin | SABIC Innovative Plastics | PEI | ULTEM™ |