Elexar® EL-1402T

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Elexar®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: FNtQKq_Elexar-EL-1402T.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
RoHS compliant halogen free flame retardant TPE
General Information
Features
  • Halogen-free
Uses
  • Cable sheath
  • Wire and cable applications
  • Wire sheath
  • Connector
  • cord sheath
  • Terminal cable sheath material
RoHS Compliance
  • RoHS compliance
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.11g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg)2.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore A, 5 sec)87ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Strength (Break)10.3MPaASTM D412
Tensile Elongation (Break)650%ASTM D412
AgingNominal ValueUnitTest Method
Change in Tensile Strength in Air ASTM D573
    136°C, 168 hr 0.0%ASTM D573
    158°C, 168 hr 3.0%ASTM D573
Change in Ultimate Elongation in Air ASTM D573
    136°C, 168 hr -5.0%ASTM D573
    158°C, 168 hr -4.0%ASTM D573
ThermalNominal ValueUnitTest Method
Brittleness Temperature < -52.0°CASTM D746
ElectricalNominal ValueUnitTest Method
Dielectric Constant ASTM D2520
    1 kHz 3.04ASTM D2520
    1 MHz 3.54ASTM D2520
Dissipation Factor ASTM D150
    1 kHz 0.016ASTM D150
    1 MHz 0.079ASTM D150
FlammabilityNominal ValueUnitTest Method
Flame Rating (3.18 mm)V-0UL 94
Oxygen Index 28%ASTM D2863
InjectionNominal ValueUnit
Rear Temperature 171 - 177°C
Middle Temperature 177 - 182°C
Front Temperature 182 - 188°C
Nozzle Temperature 188 - 193°C
Processing (Melt) Temp 188 - 193°C
Mold Temperature 25.0 - 65.6°C
Injection Pressure 1.38 - 6.89MPa
Injection Rate Moderate-Fast
Back Pressure 0.172 - 0.345MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 1 to 2 hours at 176°F (80°C).
ExtrusionNominal ValueUnit
Drying Temperature 80.0°C
Drying Time 1.0 - 2.0hr
Cylinder Zone 1 Temp. 171 - 177°C
Cylinder Zone 2 Temp. 177 - 182°C
Cylinder Zone 3 Temp. 182 - 188°C
Cylinder Zone 4 Temp. 188 - 193°C
Cylinder Zone 5 Temp. 188 - 193°C
Melt Temperature 193 - 196°C
Die Temperature 121 - 177°C
Extrusion instructions
Screw Speed: 30 to 100 rpm
Resin Grade Manufacturer Category Trademark
RTP 1105 FR RTP Company PET RTP
TEREZ PMMA 5805 SZ TER HELL PLASTIC GMBH Acrylic (PMMA) TEREZ PMMA
Adell Polyamide BT-13 Adell Plastics, Inc. Nylon 6 Adell Polyamide
AIE PC/ABS A2200FR-5008 Asia International Enterprise (Hong Kong) Limited PC+ABS AIE PC/ABS
Kumho SBR 1712G Korea Kumho Petrochemical Co., Ltd. SBR, Emulsion Kumho SBR