Category: | ABS , Acrylonitrile Butadiene Styrene |
Manufacturer: | A. Schulman Europe |
Trademark: | RONFALIN® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | FIcQHo_RONFALINVE101.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
RONFALIN®VE 101 is an acrylonitrile butadiene styrene (ABS) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is injection molding. RONFALIN®The main features of VE 101 are:
|
General Information | |
---|---|
Features |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.19 | g/cm³ | ISO 1183/A |
Melt Volume-Flow Rate (MVR) (220°C/10.0 kg) | 25.0 | cm³/10min | ISO 1133 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus | 2500 | MPa | ISO 527-2/1A/1 |
Tensile Stress | ISO 527-2/1A/50 | ||
Yield | 45.0 | MPa | ISO 527-2/1A/50 |
Fracture | 40.0 | MPa | ISO 527-2/1A/50 |
Tensile Strain (Yield) | 3.0 | % | ISO 527-2/1A/50 |
Nominal Tensile Strain at Break | 8.0 | % | ISO 527-2/1A/50 |
Flexural Modulus 1 | 2700 | MPa | ISO 178 |
Flexural Stress 2 | ISO 178 | ||
4.2% strain | 75.0 | MPa | ISO 178 |
3.5% strain | 74.0 | MPa | ISO 178 |
8.5% strain | 68.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | ||
-30°C | 6.0 | kJ/m² | ISO 179/1eA |
23°C | 11 | kJ/m² | ISO 179/1eA |
Charpy Unnotched Impact Strength | ISO 179/1eU | ||
-30°C | 45 | kJ/m² | ISO 179/1eU |
23°C | 65 | kJ/m² | ISO 179/1eU |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature | |||
0.45 MPa, not annealed | 83.0 | °C | ISO 75-2/Bf |
1.8 MPa, not annealed | 75.0 | °C | ISO 75-2/Af |
Vicat Softening Temperature | |||
-- | 102 | °C | ISO 306/A50 |
-- | 93.0 | °C | ISO 306/B50 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Comparative Tracking Index (Solution A) | 350 | V | IEC 60112 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flammability Classification | IEC 60695-11-10, -20 | ||
0.8 mm | V-0 | IEC 60695-11-10, -20 | |
1.6 mm | V-0 | IEC 60695-11-10, -20 | |
3.2 mm | V-0 | IEC 60695-11-10, -20 | |
Glow Wire Flammability Index | IEC 60695-2-12 | ||
1.5 mm | 960 | °C | IEC 60695-2-12 |
3.0 mm | 960 | °C | IEC 60695-2-12 |
Glow Wire Ignition Temperature | IEC 60695-2-13 | ||
1.5 mm | 700 | °C | IEC 60695-2-13 |
3.0 mm | 725 | °C | IEC 60695-2-13 |
Additional Information |
---|
1.) Not for use in food contact applications2.) Not for use in medical or pharmaceutical applications |
Note Message | |
---|---|
1 . | 2.0 mm/min |
2 . | 2.0 mm/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SCHULAMID® 6 GF 40 | A. Schulman Europe | Nylon 6 | SCHULAMID® |
Nipol® Roadace | Zeon Corporation | Latex | Nipol® |
Braskem PE CP 191XP | Braskem | PP Copolymer | Braskem PE |
DENILUB PA66 NEAT RESIN | Vamp Tech | Nylon 66 | DENILUB |
HiFill® PA4/6 CF30 | Techmer Engineered Solutions | Nylon 46 | HiFill® |