| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | Polykemi AB |
| Trademark: | SCANAMID 6 |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | EIdtoa_SCANAMID-6-B12-NH6.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Flame retardant halogen free |
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.14 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 1.0 to 1.2 | % | |
| Flow | 1.0 to 1.2 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 74.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 9.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 3000 | MPa | ISO 178 |
| Flexural Stress | 115 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 5.0 | kJ/m² | ISO 179 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1 | |||
| 0.45 MPa, Unannealed | 177 | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 63.0 | °C | ISO 75-2/A |
| Vicat Softening Temperature | |||
| -- | 216 | °C | ISO 306/A50 |
| -- | 200 | °C | ISO 306/B50 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (1.60 mm) | V-0 | UL 94 | |
| Glow Wire Ignition Temperature (2.00 mm) | 960 | °C | IEC 60695-2-13 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Multi-Flex® TPE D3204 | Multibase, A Dow Corning Company | TPE | Multi-Flex® TPE |
| Karina NATURAL PVC COMPOUND 900-25/1-AYR-IS (*) | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
| MAJORIS DEG387 - 8651 | AD majoris | PP, Unspecified | MAJORIS |
| P-BLEND X85 | Putsch Kunststoffe GmbH | PC+ABS | P-BLEND |
| POLYelast TPE EDS80 D35 | Polykemi AB | PP+EPDM | POLYelast |