Category: | TPU-Polyether , Thermoplastic Polyurethane Elastomer (Polyether) |
Manufacturer: | API SpA |
Trademark: | apilon 52® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | EC3yeX_apilon-52-TL-62.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
apilon 52®TL 62 is a thermoplastic polyurethane elastomer (polyether)(TPU-polyether) product,. It can be processed by injection molding and is available in Europe. apilon 52®The application areas of TL 62 include engineering/industrial accessories, electrical/electronic applications, electrical appliances, tools and home applications. Features include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.17 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D, 3 sec) | 62 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | ASTM D638 | ||
-- | 40.0 | MPa | ASTM D638 |
100% strain | 18.0 | MPa | ASTM D638 |
300% strain | 30.0 | MPa | ASTM D638 |
Tensile Elongation (Break) | 400 | % | ASTM D638 |
Flexural Modulus | 200 | MPa | ASTM D790 |
Abrasion Resistance | 50.0 | mm³ | DIN 53516 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tear Strength 1 | 150 | kN/m | ASTM D624 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (-20°C) | No Break | ASTM D256 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 110 | °C | |
Drying Time | 2.0 | hr | |
Suggested Max Moisture | 0.070 | % | |
Rear Temperature | 180 - 190 | °C | |
Middle Temperature | 185 - 200 | °C | |
Front Temperature | 190 - 215 | °C | |
Nozzle Temperature | 200 - 230 | °C | |
Mold Temperature | 30.0 - 60.0 | °C | |
Injection Pressure | 50.0 - 100 | MPa | |
Injection Rate | Slow-Moderate |
Injection instructions |
---|
Back Pressure: Medium to LowLocking Pressure: High |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 - 110 | °C | |
Drying Time | 2.0 | hr | |
Suggested Max Moisture | 0.070 | % | |
Cylinder Zone 1 Temp. | 160 - 185 | °C | |
Cylinder Zone 2 Temp. | 170 - 200 | °C | |
Cylinder Zone 3 Temp. | 175 - 210 | °C | |
Cylinder Zone 4 Temp. | 180 - 220 | °C | |
Die Temperature | 170 - 210 | °C |
Extrusion instructions |
---|
L/D Ratio: 20:1 to 30:1Compression Ratio: 1:2.5 to 1:3 |
Note Message | |
---|---|
1 . | Without Notch |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Shin-Etsu Elastomer KE-2004-5A/B | Shin-Etsu Silicones of America | Silicone Rubber, HTV | Shin-Etsu Elastomer |
Tecotek® PC43 GR003 TD70 | Eurotec Engineering Plastics | PC | Tecotek® |
VYLOPET® EMC605P | TOYOBO America, Inc. | PBT+PET | VYLOPET® |
DiaAlloy FC-304G | Mitsubishi Rayon America Inc. | PC | DiaAlloy |
Star T PA6 65E12 | Eurostar Engineering Plastics | Nylon 6 | Star T |