| Category: | PP Homopolymer , Polypropylene Homopolymer |
| Manufacturer: | Polykemi AB |
| Trademark: | POLYfill |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | E9dlHi_POLYfill-PPH-GK8040.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass reinforced |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.21 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 8.0 | g/10 min | ISO 1133 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 0.80 to 1.2 | % | |
| Flow | 0.80 to 1.2 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | 30.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield) | 6.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 2800 | MPa | ISO 178 |
| Flexural Stress | 50.0 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 3.0 | kJ/m² | ISO 179 |
| Charpy Unnotched Impact Strength (23°C) | 15 | kJ/m² | ISO 179 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 1 | |||
| 0.45 MPa, Unannealed | 120 | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 65.0 | °C | ISO 75-2/A |
| Vicat Softening Temperature | |||
| -- | 150 | °C | ISO 306/A50 |
| -- | 90.0 | °C | ISO 306/B50 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RASCHIG EN 5004/5007 | RASCHIG GmbH | Epoxy | RASCHIG |
| BFI 428 | Blueridge Films Inc. | HDPE | BFI |
| Anjacom® 055/80-GK20 | Almaak International GmbH | PC+ABS | Anjacom® |
| Halar® 930LCW | Solvay Specialty Polymers | ECTFE | Halar® |
| LEXAN™ EXL1890T resin | SABIC Innovative Plastics | PC | LEXAN™ |