TECHNYL STAR™ AF 219 V30 BLACK

Category: Nylon 66 , Polyamide 66
Manufacturer: Solvay Engineering Plastics
Trademark: TECHNYL STAR™
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: E99GzO_TECHNYL-STAR-AF-219-V30-BLACK.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
TECHNYL STAR™ AF 219 V30 BLACK is a Polyamide 66 (Nylon 66) material filled with 30% glass fiber. It is available in Europe for injection molding.

Important attributes of TECHNYL STAR™ AF 219 V30 BLACK are:
  • RoHS Compliant
  • Good Aesthetics
  • Good Processability
  • Heat Stabilizer
  • High Flow

Typical applications include:
  • Electrical/Electronic Applications
  • Engineering/Industrial Parts
  • Wire & Cable
General Information
Filler / Reinforcement
  • Glass Fiber, 30% Filler by Weight
Additive
  • Heat Stabilizer
Features
  • Good Processability
  • Good Surface Finish
  • Heat Stabilized
  • High Flow
Uses
  • Connectors
  • Electrical/Electronic Applications
  • Insulation
  • Thin-walled Parts
Agency Ratings
  • UU 453/2010/EC
RoHS Compliance
  • RoHS Compliant
Appearance
  • Black
Processing Method
  • Injection Molding
Part Marking Code (ISO 11469)
  • >PA66-GF30<
PhysicalNominal ValueUnitTest Method
Density 1.37g/cm³ISO 1183/A
Molding Shrinkage Internal Method
    Across Flow 0.80%
    Flow 0.50%
Water Absorption (23°C, 24 hr)0.80%ISO 62
Molding Shrinkage Isotropy 0.620Internal Method
MechanicalNominal ValueUnitTest Method
Tensile Modulus 10000MPaISO 527-2/1A
Tensile Stress (Break)190MPaISO 527-2/1A
Tensile Strain (Break)3.0%ISO 527-2/1A
Flexural Modulus 9000MPaISO 178
Flexural Stress 270MPaISO 178
ImpactNominal ValueUnitTest Method
Charpy Notched Impact Strength 10kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength 70kJ/m²ISO 179/1eU
ThermalNominal ValueUnitTest Method
Heat Deflection Temperature
    0.45 MPa, Unannealed 258°CISO 75-2/Bf
    1.8 MPa, Unannealed 250°CISO 75-2/Af
Melting Temperature 263°CISO 11357-3
CLTE - Flow (23 to 85°C)2.5E-5cm/cm/°CISO 11359-2
ElectricalNominal ValueUnitTest Method
Comparative Tracking Index (Solution A)600VIEC 60112
InjectionNominal ValueUnit
Drying Temperature 80.0°C
Suggested Max Moisture 0.20%
Rear Temperature 260 to 270°C
Middle Temperature 270 to 280°C
Front Temperature 280 to 290°C
Mold Temperature 60.0 to 80.0°C
Resin Grade Manufacturer Category Trademark
Generic PP Terpolymer Generic PP Terpolymer Generic
Hostacom TRC 333N LyondellBasell Industries Polyolefin, Unspecified Hostacom
ORIENTENE FM 08 Oriental Petrochemical Company PP Homopolymer ORIENTENE
apilon 52® A-52/40 API SpA TPU-Polyester apilon 52®
EPALINE 786A34 Epaflex Polyurethanes S.R.L. TPU-Polyether EPALINE